THEORY OF DYNAMIC OPTIMIZATION FOR MATERIALS HEATING PROCESS——CRITERION RESTRAINING METHOD
LI Zongrui;LU Zhongwu Northeast University of Technology; Shenyang
Cite this article: 

LI Zongrui;LU Zhongwu Northeast University of Technology; Shenyang. THEORY OF DYNAMIC OPTIMIZATION FOR MATERIALS HEATING PROCESS——CRITERION RESTRAINING METHOD. Acta Metall Sin, 1992, 28(4): 45-48.

Download:  PDF(430KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A criterion restraining method adopted to the dynamic optimization for materi-als heating process has been developed, regarding it as controlled object of a regulator in controltheory and combining the optimal criterion of it. The method may be available to optimize fuelsupply along furnace length and to provide a theoretical basis for the optimization of fuel supplyin time-varying. For soaking pit, the calculation shows that in case of optimization by criterionrestraining method, the thermal efficiency is 3.1% higher than the modelling prediction result.In comparison with heat flux-decomposing method, the thermal efficiency increased from 43.1to 43.8%, and the energy consumption was reduced by 7.28% relative to the practical produc-tion data.
Key words:  optimization      heating process      control theory      optinal criterion     
Received:  18 April 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I4/45

1 Misaka Y, Takahashi R, Shinjo A, Nariai Y, Kooriki M. Iron Steel Eng, 1982; 59(5) : 51
2 Schurko R J, Weinstein C, Hanne M K, Pellecchia D J, Iron Steel Eng, 1987; 64(5) : 37
3 Doi K, Shinmura T, Ohnishi T, Kawasumi T. Automation in Mining, Mineral and Metal Processing, Helshinki, Finland, 1983: 39
4 Kohlgrueber K, Woelk G. Gas Waerme Int, 1985; 34: 418
5 李宗瑞,陆钟武.金属学报,1991;27:B1
6 谢绪恺.现代控制理论基础.沈阳:辽宁人民出版社,1980:341
7 Hottel H C. J Inst Fuel, 1961; (6) : 220
[1] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[2] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[3] ZHAO Wanchen, ZHENG Chen, XIAO Bin, LIU Xing, LIU Lu, YU Tongxin, LIU Yanjie, DONG Ziqiang, LIU Yi, ZHOU Ce, WU Hongsheng, LU Baokun. Composition Refinement of 6061 Aluminum Alloy Using Active Machine Learning Model Based on Bayesian Optimization Sampling[J]. 金属学报, 2021, 57(6): 797-810.
[4] SUN Xiaofeng, SONG Wei, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Research and Development in Materials and Processes of Superalloy Fabricated by Laser Additive Manufacturing[J]. 金属学报, 2021, 57(11): 1471-1483.
[5] SHENG Ying, JIA Bin, WANG Ruheng, CHEN Guoping. The Definition of Atomic Scale Strain and Its Application in Identifying the Evolution of Microdefects[J]. 金属学报, 2020, 56(8): 1144-1154.
[6] WANG Fuqiang, LIU Wei, WANG Zhaowen. Effect of Local Cathode Current Increasing on Bath-Metal Two-Phase Flow Field in Aluminum Reduction Cells[J]. 金属学报, 2020, 56(7): 1047-1056.
[7] TANG Haiyan, LI Xiaosong, ZHANG Shuo, ZHANG Jiaquan. Fluid Flow and Heat Transfer in a Tundish with Channel Induction Heating for Sequence Casting with a Constant Superheat Control[J]. 金属学报, 2020, 56(12): 1629-1642.
[8] Tongxiang FAN, Yue LIU, Kunming YANG, Jian SONG, Di ZHANG. Recent Progress on Interfacial Structure Optimization and Their Influencing Mechanism of Carbon Reinforced Metal Matrix Composites[J]. 金属学报, 2019, 55(1): 16-32.
[9] WANG Dapeng WANG Dazhi WU Baolin ZUO Liang WANG Fu LIANG Zhide. IMPROVEMENT ON THE MODIFIED MAXIMUM ENTROPY METHOD FOR TEXTURE ANALYSIS BY PARTICLE SWARM OPTIMIZATION[J]. 金属学报, 2009, 45(1): 63-66.
[10] . Modeling and optimization of movement parameters of reciprocating tubular spray depositing[J]. 金属学报, 2008, 44(4): 501-506 .
[11] ;. Applying Particle Swarm Optimization to The Quantitative Texture Analysis based on Maximum Entropy Method[J]. 金属学报, 2008, 44(2): 183-187 .
[12] WANG Xiaoying; ZHANG Ruijie; JIE Wanqi. DISSOLUTION OF THE SECOND PHASE DURING CONTINUOUS HEATING PROCESS[J]. 金属学报, 2004, 40(4): 434-438 .
[13] CHE Hiaozhou(Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1994-12-09; in revised forrn 1995-03-27). STRESS RELIEF AND MAGNETISM OPTIMIZATION OF AMORPHOUS Fe_(79)B_(16)Si_5 ALLOY[J]. 金属学报, 1995, 31(21): 418-422.
[14] ZHA NG Peixin; ZHA NG Qizhi; W U Liming; SUI Zhitong(Northeasiern Unirersity.Shenyang 110006). OPTIMIZATION OF MgO-B_2O_3-SiO_2 SLAGGING USING ARTIFICIAL NEURAL NETWORK AND GENETIC ALGORITHM[J]. 金属学报, 1995, 31(18): 284-288.
[15] LI Zongrui;LU Zhongwu Northeast University of Technology; Shenyang. ON THE CRITERION AND THEORY OF OPTIMIZATION IN HEATING PROCESS OF MATERIALS[J]. 金属学报, 1991, 27(1): 78-82.
No Suggested Reading articles found!