THERMODYNAMIC PROPERTIES OF HOLE TRAPS A AND B IN GaAs
FU Zhiping;LU Dongliang;ZHAN Qianbao;ZHOU Jicheng Shanghai Institute of Metallurgy; Academia Sinica; Correspondent professor; Shanghai Institute of MetaHurgy; Academia Sinica; Shanghai 20050
Cite this article: 

FU Zhiping;LU Dongliang;ZHAN Qianbao;ZHOU Jicheng Shanghai Institute of Metallurgy; Academia Sinica; Correspondent professor; Shanghai Institute of MetaHurgy; Academia Sinica; Shanghai 20050. THERMODYNAMIC PROPERTIES OF HOLE TRAPS A AND B IN GaAs. Acta Metall Sin, 1992, 28(5): 59-63.

Download:  PDF(402KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Equilibrium constant, K_T, and free energy of formation △G, of the reaction: Ga_(As)As_(Ga)+(V_(Ga))_2~-+e~-=As_(Ga)V_(Ga)~-+Ga_(As)V_(Ga)~-were deduced as: K_T=(1.088×10~81.090×10~(11)·1/ T)~2 AG°=-2RTln(1.088×10~8-1.090×10~(11)·1/ T) These seem to be applicable into practice under certain conditions.
Key words:  GaAs      hole trap      thermodynamic property     
Received:  18 May 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I5/59

1 邹元燨.全国微波技术会议,石家庄,1974
2 Long D V, Logan R A. J Electron Mater, 1975; 4: 1053
3 邹元燨.见:全国砷化镓及其它Ⅲ-Ⅴ族化合物半导体会议文集,柳州,1977:48
4 Zhou Jicheng, Luo Yian, Li Liansheng, Lu Bingfang, Zhang Jue. Mater Lett, 1987; 5: 479
5 Zhou Jicheng, Li Liansheng, Liu Miaoxiu, Lu Bingfang, Zhang Jue. Mater Lett, 1987; 6: 247
6 Zhou Jicheng, Luo Yian, Lu Bingfang, Zhan Qianbao. Mater Lett, 1988; 7: 391
7 Tegude F J, Baston J, Arnold N, Heime K. In: Persented at 2nd conf on Si Ⅲ-Ⅴ Materials, Evian, France, 1982
8 Chiang S Y, Pcarson G L. J Appl Phys, 1975; 46: 2986
9 Zou Y, Zhou J, Lu Y, Wang G, Hu B, Li C, Li L, Shao J, Sheng C. J Electron Mater, 1985; 14A: 1021
10 Zhou Jicheng, Fu Zhiping, Zhan Qianbao, Feng Shuifu. In: Swaminathan V, Manasreh O, Pearton S J eds., Proc MRS Spring Meeting, Vol. 184, Pittsburgh, PA: Materials Research Society, 1990: 68
11 李爱珍,潘慧珍,杨倩志,唐嫱妹,邱建华,曹自立,陈国建.见:全国砷化镓及其它Ⅲ-Ⅴ族化合物半导体会议文集,柳州,1977:54
[1] HUANGFU Hao, WANG Zilong, LIU Yongli, MENG Fanshun, SONG Jiupeng, QI Yang. A First Principles Investigation of W1 - x Ir x Alloys: Structural, Electronic, Mechanical, and Thermal Properties[J]. 金属学报, 2022, 58(2): 231-240.
[2] Ronghua CUI, Xinyu WANG, Zhengchao DONG, Chonggui ZHONG. First Principles Study on Elastic and Thermodynamic Properties of Mg1-xZnx Alloys[J]. 金属学报, 2017, 53(9): 1133-1139.
[3] ZHANG Xudong, WANG Shaoqing. FIRST-PRINCIPLES INVESTIGATION OF THE THERMODYNAMICS PROPERTIES OF Al3Sc AND Al3Zr INTERMETALLICS[J]. 金属学报, 2013, 29(4): 501-505.
[4] WEI Bingbo; DONG Changxing(Northwestern Polytechnical University; Xi'an 710072)(Manuscript received 1995-09-25). HYPERCOOLING AND THERMODYNAMIC PROPERTIES OF LIQUID Ni-Fe ALLOYS[J]. 金属学报, 1996, 32(4): 357-362.
[5] ZENG Wenming;CHEN Nianyi(Shanghai Institute of Metallurgy;Chinese Academy of Sciences;Shanghai 200050);YE Dalun(Kunming University of Science and Technology; Kunming 650093)(Manuscript received 1995-10-24;in revised form 1996-08-13). THERMODYNAMIC PROPERTIES OF Sn-Sb ALLOYS[J]. 金属学报, 1996, 32(12): 1233-1237.
[6] CHEN Qiyuan; ZENG Wenming; ZHANG Pingmin (Central-South University of Technology; Changsha 410083)GU Songqing; YANG Guanqun; ZHOU Huifang; YIN Zhonglin (Zhengzhou Research institute of Light Metals; Zhengzhou 450041) (Manuscript received 1995-02-23; in revised form 1995-06-29). THERMODYNAMIC PROPERTIES OF SOME ALUMINUM COMPOUNDS[J]. 金属学报, 1996, 32(1): 6-14.
[7] XU Qian;YU Yaxin;QIU Zhuxian(Northeastern University;Shenyang)(Manuscript received 25 June;1993). THERMODYNAMIC PROPERTIES AND PHASE DIAGRAMS OF Li-CaF_2,NaF-CaF_2 AND KF-CaF_2[J]. 金属学报, 1994, 30(16): 150-155.
[8] XU Qian;QIU Zhuxian Northeast University of Technology; Shenyang. CALCULATION OF THERMODYNAMIC PROPERTIES OF LiF-AlF_3 MELTS[J]. 金属学报, 1993, 29(9): 60-64.
[9] TAO Dongping Kunming Institute of Technology. PREDICTION ABOUT THERMODYNAMIC PROPERTIES OF TERNARY LIQUID ALLOYS FROM WILSON EQUATION[J]. 金属学报, 1991, 27(6): 92-98.
[10] XU Chi;JIANG Naixiong;CHEN Nianyi Shanghai Institute of Metallurgy; Academia sinica. THERMODYNAMICS OF COMPUTERIZED SIMULATION OF MOLTEN LIF-KF SOLUTION BY MONTE CARLO METHOD[J]. 金属学报, 1991, 27(5): 144-147.
[11] LI Guodong;DU Ting Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing. THERMODYNAMIC PROPERTIES OF Cu-Ce-S AND Cu-Y-S LIQUID SOLUTIONS[J]. 金属学报, 1991, 27(4): 142-144.
No Suggested Reading articles found!