| THERMODYNAMIC PROPERTIES OF HOLE TRAPS A AND B IN GaAs |
| FU Zhiping;LU Dongliang;ZHAN Qianbao;ZHOU Jicheng Shanghai Institute of Metallurgy; Academia Sinica; Correspondent professor; Shanghai Institute of MetaHurgy; Academia Sinica; Shanghai 20050 |
|
Cite this article:
FU Zhiping;LU Dongliang;ZHAN Qianbao;ZHOU Jicheng Shanghai Institute of Metallurgy; Academia Sinica; Correspondent professor; Shanghai Institute of MetaHurgy; Academia Sinica; Shanghai 20050. THERMODYNAMIC PROPERTIES OF HOLE TRAPS A AND B IN GaAs. Acta Metall Sin, 1992, 28(5): 59-63.
|
|
|
Abstract Equilibrium constant, K_T, and free energy of formation △G, of the reaction: Ga_(As)As_(Ga)+(V_(Ga))_2~-+e~-=As_(Ga)V_(Ga)~-+Ga_(As)V_(Ga)~-were deduced as: K_T=(1.088×10~81.090×10~(11)·1/ T)~2 AG°=-2RTln(1.088×10~8-1.090×10~(11)·1/ T) These seem to be applicable into practice under certain conditions.
|
|
Received: 18 May 1992
|
1 邹元燨.全国微波技术会议,石家庄,1974 2 Long D V, Logan R A. J Electron Mater, 1975; 4: 1053 3 邹元燨.见:全国砷化镓及其它Ⅲ-Ⅴ族化合物半导体会议文集,柳州,1977:48 4 Zhou Jicheng, Luo Yian, Li Liansheng, Lu Bingfang, Zhang Jue. Mater Lett, 1987; 5: 479 5 Zhou Jicheng, Li Liansheng, Liu Miaoxiu, Lu Bingfang, Zhang Jue. Mater Lett, 1987; 6: 247 6 Zhou Jicheng, Luo Yian, Lu Bingfang, Zhan Qianbao. Mater Lett, 1988; 7: 391 7 Tegude F J, Baston J, Arnold N, Heime K. In: Persented at 2nd conf on Si Ⅲ-Ⅴ Materials, Evian, France, 1982 8 Chiang S Y, Pcarson G L. J Appl Phys, 1975; 46: 2986 9 Zou Y, Zhou J, Lu Y, Wang G, Hu B, Li C, Li L, Shao J, Sheng C. J Electron Mater, 1985; 14A: 1021 10 Zhou Jicheng, Fu Zhiping, Zhan Qianbao, Feng Shuifu. In: Swaminathan V, Manasreh O, Pearton S J eds., Proc MRS Spring Meeting, Vol. 184, Pittsburgh, PA: Materials Research Society, 1990: 68 11 李爱珍,潘慧珍,杨倩志,唐嫱妹,邱建华,曹自立,陈国建.见:全国砷化镓及其它Ⅲ-Ⅴ族化合物半导体会议文集,柳州,1977:54 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|