Please wait a minute...
Acta Metall Sin  1992, Vol. 28 Issue (5): 51-58    DOI:
Current Issue | Archive | Adv Search |
A COMPOSITE METHOD OF SOLUTION FOR CONTACT STRESSES ON ROLLER
QU Zhihao;PENG Huihong Shanghai Technical College of Metallurgy; Shanghai Institute of Non-Ferrous Metals;Correspondent Faculty of Mechamics; Shanghai Technical College of Metalhurgy; Shanghai 200233
Cite this article: 

QU Zhihao;PENG Huihong Shanghai Technical College of Metallurgy; Shanghai Institute of Non-Ferrous Metals;Correspondent Faculty of Mechamics; Shanghai Technical College of Metalhurgy; Shanghai 200233. A COMPOSITE METHOD OF SOLUTION FOR CONTACT STRESSES ON ROLLER. Acta Metall Sin, 1992, 28(5): 51-58.

Download:  PDF(986KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A composite method of solution for contact stresses on roller was suggested bythe combination of similitude principle, photoelastic method, Hertz's contact theoty andnumerical calculation. Thus, not only the reasonable distribution of axial contact pressureon roller of limited Iength, but also the three-dimensional solution of stress in the contactpost may be obtained. Obeservation on the prachcal damaged roller is in agreement with theresult after contact stress analysis of such a working roller.
Key words:  roller      contact stress      similitude principle      photoelastic stress     
Received:  18 May 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I5/51

1 徐芝纶.弹性力学.北京:人民教育出版社,1979:240--264,287--294
2 天津大学材料力学教研室光弹组主编.光弹性原理及测试技术.北京:科学出版社,1980:416--425
3 Kabayashi A S. Handbook on Experimental Machanics. Englewood: Prentice-Hall, 1987: 105--131
[1] Zhiqiang ZHANG,Limin DONG,Shaoxuan GUAN,Rui YANG. Microstructure and Mechanical Properties of TC16 Titanium Alloy by Room Temperature Roller Die Drawing[J]. 金属学报, 2017, 53(4): 415-422.
[2] LIU Chaosan;SHI Changxu Institute of Metal Research; Academia Sinica; ShenyangZHANG Yongchang;professor;Institute of Metal Research.Academia Sinica;Shenyang 110015. NEW AMORPHOUS AI-La-Y-Ni(Fe) QUARTERNARY ALLOYS WITH SUPERIOR STRENGTH AND DUCTILITY[J]. 金属学报, 1993, 29(6): 66-70.
[3] WEI Dezhou;SUN Yubo Northeast University of Technology; Shenyang WEI Dezhou;lecturer;Department of Mineral Engineering;Northeast University of Techhnology;110006 Shenyang. APPLICABILITY OF SIMILITUDE PRINCIPLE TO STUDY STRATIFICATION THEORY OF GRAVITY CONCENTRATION[J]. 金属学报, 1989, 25(5): 99-106.
No Suggested Reading articles found!