Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (10): 82-86    DOI:
Current Issue | Archive | Adv Search |
MAGNETIC PROPERTIES OF NEW NANOCRYSTALLINEFe_(71.5)(CuCrV)_(7.5)Si_(12)B_9 SOFT MAGNETIC ALLOY
ZHANG Yanzhong Shanghai Iron and Steel Research Institute; Shanghai
Cite this article: 

ZHANG Yanzhong Shanghai Iron and Steel Research Institute; Shanghai. MAGNETIC PROPERTIES OF NEW NANOCRYSTALLINEFe_(71.5)(CuCrV)_(7.5)Si_(12)B_9 SOFT MAGNETIC ALLOY. Acta Metall Sin, 1993, 29(10): 82-86.

Download:  PDF(386KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In the present paper, the synthetical soft magnetic properties are reported fornewly-developed nanocrystalline Fe_(7l.5)(CuCrV)_(7.5)Si_(12)B_9 alloy. The levels of the typical mag-netic properties achieved in this new alloy are as follows. D.C. initial permeability μ_i=10.9×10~4, coercivity H_c= 0.56A/m, flux density B_80=1.04 T corresponding to H_m=80A/m;under the condition of the constant H_m=0.08A/m, a.c. effective permeability μ_e= 2.5×10~4 and 0.4×10~4 corresponding to f=0.1 and 1 MHz, respectively; core lossesP_2/100_k=195kW/m~3, P_2/200k=664kW/m~3, P_2/500k=3349kW/m~3 and P_(0.5)/1000k=720kW/m~3. The high-frequency core losses of the new alloy clearly are lower than thoseof Fe-Cu-Nb-Si-B nanocrystalline alloys and much lower than those of the superior powerMn-Zn ferrite H_(7C4). The application of the new alloy to switched mode power supply is also
Key words:  nanocrystalline alloy      relative effective permeability      relative pulse permeability      core loss      Fe_(71.5)(CuCrV)_(7.5)Si_(12)B_9     
Received:  18 October 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I10/82

1 Yoshizawa Y, Yamauchi K. IEEE Trans Magn, 1989; MAG--25: 3324
2 张延忠,年素珍.金属学报,1992;28(6) :B264-272
3 吉沢克仁,山内清隆,小熊繁.公开特许公报,昭64-79342
4 柴崎胜弘.电子技术,1989;31(8) :116-119
[1] WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping. Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects[J]. 金属学报, 2021, 57(4): 403-412.
[2] Yaoxiang GENG,Xin LIN,Jianbing QIANG,Yingmin WANG,Chuang DONG. Dual-Cluster Characteristic and Composition Optimization of Finemet Soft Magnetic Nanocrystalline Alloys[J]. 金属学报, 2017, 53(7): 833-841.
[3] CHAO Yuesheng, WANG Li, ZHANG Yanhui, ZHU Hanxian, LUO Liping. EFFECT OF LOW-TEMPERATURE VACUUM ANNEALING ON THE MAGNETIC PULSED AMORPHOUS Fe52Co34Hf7B6Cu1 ALLOY[J]. 金属学报, 2012, 48(6): 749-752.
[4] LI Dingpeng SONG Xiaoyan ZHANG Zhexu LU Nianduan QIAO Yinkai LIU Xuemei. PREPARATION AND PROPERTIES OF SINGLE–PHASE Sm5Co2 NANOCRYSTALLINE ALLOY[J]. 金属学报, 2012, 48(10): 1248-1252.
[5] LIANG Haining SONG Xiaoyan ZHANG Zhexu LU Nianduan LIU Xuemei ZHANG Jiuxing. PREPARATION AND CHARACTERIZATION OF SmCo2 NANOCRYSTALLINE ALLOY WITH PERMANENT MAGNETIC PROPERTIES[J]. 金属学报, 2010, 46(8): 973-978.
[6] WANG Zhi;HE Kaiyuan;YIN Jun;ZHANG Yumei;ZHANG LuO;LIANG Zhide (Department of Material Science and Engineering; Northeastern University; Shenyang 110006)(Institute of Materials Physics; Tianjin Institute of Technology; Tianjin 300191)(Shanghai Iron and Steel Research Institute; Shanghai 200940). TEMPERATURE DEPENDENCE OF PERMEABILITY FOR Fe-Cu-Nb-V-Si-B NANOCRYSTALLINE ALLOY[J]. 金属学报, 1998, 34(2): 200-204.
[7] DAI Wenmin;YIN Hong;YE Minjun(University of Science and Technology Beijing;Beijing 100083)(Manuscript received 1995-10-23). FRACTAL STRUCTURE OF THE CORE LOSS SPECTRUM OF SOFT MAGNETIC ALLOY WITH CONSTANT PERMEABILITY[J]. 金属学报, 1996, 32(7): 769-773.
[8] PING Dehai;QIN Hiaoying;LI Douxing;ZHANG Lide;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Institute of Solid State Physics;Chinese Academy of Sciences;Hefei 230031)(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-12-25). A MICROSTRUCTURAL EVOLUTION OF Ag-Cu NANOCRYSTALLINE ALLOYS[J]. 金属学报, 1996, 32(10): 1087-1092.
[9] ZHANG Yanzhong; (Shanghai Iron and Steel Research Institute; ShanHhai 200940) NIAN Suzhen; JIN Huijuan; XU Guiqin (Shanghai Iron and STeel Research Instituie; Shanghai 200940 ); YANG XielonK; LI Xiangqing(East China Normal University; Shanghai 200062). MAGNETIC PROPERTIES OF NANOCRYSTALLINE Fe_(74.7-X)Cu_1Nb_xV_(1.8)Si_(13.5)B_9 ALLOYS[J]. 金属学报, 1995, 31(17): 212-219.
[10] PING Dehai; (Laborutory of Atornic Imaging of Solids; Inslitute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) XIE Miansheng; JIN Zhixiong; LI Douxing; YE HenKqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research; Cthinese Academy of Sciences; Shenyang 110015). PREPARATION AND PROPERTIES OF NANOCRYSTALLINE Ti_(70)Ni_(20)Si_(10) ALLOY[J]. 金属学报, 1995, 31(17): 200-205.
[11] LU Zhichao; XIANYU Ze (Department of Physics; Northeastern University;Shenyang)SHEN Baogen((Institute of Physics; Chinese Academy of Scicnces;Beijing)LU Manqi(Institute of Metal Research; Chinese Academy of Sciences;Shenyang). THERMAL EXPANSION AND MAGNETIC PROPERTIES OF NANOCRYSTALLINE Fe-Zr-B ALLOYS[J]. 金属学报, 1994, 30(18): 265-269.
[12] BAI Kuichang;JIANG Ziying;HE Kaiyuan;CHENG Lizhi;ZHI Jing(Northeastern University;Shenyang)(Manuscript received 7 June;1993;in revised form 9 August;1993). STRUCTURAL STUDY OF NANOCRYSTALLINE Fe-Cu-Nb-Si-B ALLOYS BY MSSBAUER SPECTROSCOPY[J]. 金属学报, 1994, 30(14): 66-71.
[13] ZHI Jing;HE Kaiyuan;CHENG Lizhi;FU Yujun;WANG Zhi;LIU Yi (Northeastern University;Shengyang)(Manuscript received 30 January 1993:in revised form 25 June;1993). MICROSTRUCTURE AND MAGNETIC PROPERTIES OF NANOCRYSTALLINE(Fe,Cu,Nb)_(77.5)Si_xB_(22.5-x) ALLOYS[J]. 金属学报, 1994, 30(14): 61-65.
[14] LIU Xuedong;ZHU Jie;JIANG Jian;DING Bingzhe;WANG Jingtang Institute of Metal Research. Academia Sinica; Shenyang. STRUCTURE OF NANOCRYSTALLINE Fe-Cu-Si-B ALLOYS[J]. 金属学报, 1993, 29(9): 72-76.
[15] TONG Huayu;DING Bingzhe;JIANG Honggang;LI Shuling;LI Gusong;WANG Jingtang State Key Laboratory of RSA; Institute of Metal Research; Academia Sinica; Shenyang Correspondent Research assistant; Institute of Metal Research; Academia Sinica; Shenyang 110015. THERMAL PROPERTIES OF NANOCRYSTALLINE Fe_(78)B_(13)Si_9 ALLOY[J]. 金属学报, 1992, 28(6): 71-75.
No Suggested Reading articles found!