| REDUCTION OF da/dN AT DIFFERENT SHOCK WAVE AFFECTING REGIONS |
| CHEN Liangshan;SI Zhongyao;TAN Shengyu;CUI Guangyuan Institute of Metal Research; Academia Sinica; Shenyang Shenyang Institute of AritilleryCHEN Huaining;research associate;Institute of Metal Research Academia Sinica;Shenyang 110015 |
|
Cite this article:
CHEN Liangshan;SI Zhongyao;TAN Shengyu;CUI Guangyuan Institute of Metal Research; Academia Sinica; Shenyang Shenyang Institute of AritilleryCHEN Huaining;research associate;Institute of Metal Research Academia Sinica;Shenyang 110015. REDUCTION OF da/dN AT DIFFERENT SHOCK WAVE AFFECTING REGIONS. Acta Metall Sin, 1993, 29(6): 38-42.
|
|
|
Abstract Changes of fatigue crack growth rate, dα/dN, at affecting region of eitherplastic or elastic shock wave have been studied with three-point bending specimens made oflow alloy steel 16Mn. The dα/dN at whole affecting regions by shock wave, about 100 mmdepth, is significantly reduced, especially at the plastic wave affecting region. Thedα/dN keeps basically constant at pure elastic wave affecting region under same ΔK. It isconsidered that the decrease of effective stress intensity factor ΔK_(eff) of the material with crackclosure effect is the main reason for reducing dα/dN after shock wave treatment. At plasticwave affecting region, crack closure occurs mainly through plastic deformations at crack tipand oxides; at elastic wave affecting region, through plastic deformations and roughness.
|
|
Received: 18 June 1993
|
1 高桦.固体力学学报,1987;(2) :164 2 斯重遥,陈亮山,刘易军.第6届全国焊接学术会议论文集,西安,1990 3 陈怀宁,陈亮山,斯重遥.第5届沈阳市焊接学术会议论文集.1991 4 北京工业学院.爆炸及其作用下册.北京:国防工业出版社,1979:180 5 赵铁民,陈亮山,陈怀宁.斯重遥.第七届全国焊接学术会议论文集,青岛,1993< |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|