| INTERNAL OXIDATION OF Pd-Eu ALLOYS |
| NING Yuantao;WEN Fei;ZHAO Huaizhi;DENG Deguo Kunming Institute of Precious Metals |
|
Cite this article:
NING Yuantao;WEN Fei;ZHAO Huaizhi;DENG Deguo Kunming Institute of Precious Metals. INTERNAL OXIDATION OF Pd-Eu ALLOYS. Acta Metall Sin, 1993, 29(9): 65-71.
|
|
|
Abstract The internal oxidation of active solute Eu in Pd-Eu alloys has been studied inair at 800--1200℃. It was a nucleation and growing process of stable oxide Eu_2O_3 controlledby diffusion mechanism: oxygen entered to internal layer and Eu diffused towards outer layerand surface through bulk and grain boundary diffusion, this caused non-homogeneous dis-tribution of oxygen and Eu. For wire samples with dia. 2mm, the dependence of the internaloxidation depth (ξ) on the reaction time (t) could be expressed as ξ= Kt~n, here n=0.5 at 800--900℃, and n=0.75 at 1200℃. The activation energy of Pd-0.56at.-%Eu alloy was deter-mined to be 150 kJ/mol.
|
|
Received: 18 September 1993
|
1 宁远涛,李永年.金属学报,1989;25:B16 2 冯端.金属物理学(第一卷).北京:科学出版社,1987:317 3 Ning Yuantao, Li Yongnian, Dai Hong. Rare Metals, 1990; 9(1) :30 4 Charrin L. Combe A, Moya G. Acta Metall, 1981; 29: 1593q |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|