INTERNAL OXIDATION OF Pd-Eu ALLOYS
NING Yuantao;WEN Fei;ZHAO Huaizhi;DENG Deguo Kunming Institute of Precious Metals
Cite this article: 

NING Yuantao;WEN Fei;ZHAO Huaizhi;DENG Deguo Kunming Institute of Precious Metals. INTERNAL OXIDATION OF Pd-Eu ALLOYS. Acta Metall Sin, 1993, 29(9): 65-71.

Download:  PDF(2590KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The internal oxidation of active solute Eu in Pd-Eu alloys has been studied inair at 800--1200℃. It was a nucleation and growing process of stable oxide Eu_2O_3 controlledby diffusion mechanism: oxygen entered to internal layer and Eu diffused towards outer layerand surface through bulk and grain boundary diffusion, this caused non-homogeneous dis-tribution of oxygen and Eu. For wire samples with dia. 2mm, the dependence of the internaloxidation depth (ξ) on the reaction time (t) could be expressed as ξ= Kt~n, here n=0.5 at 800--900℃, and n=0.75 at 1200℃. The activation energy of Pd-0.56at.-%Eu alloy was deter-mined to be 150 kJ/mol.
Key words:  Palladium alloy      Eu additive      internal oxidation     
Received:  18 September 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I9/65

1 宁远涛,李永年.金属学报,1989;25:B16
2 冯端.金属物理学(第一卷).北京:科学出版社,1987:317
3 Ning Yuantao, Li Yongnian, Dai Hong. Rare Metals, 1990; 9(1) :30
4 Charrin L. Combe A, Moya G. Acta Metall, 1981; 29: 1593q
[1] PING Faping, HU Qingmiao, YANG Ru. INVESTIGATION ON EFFECTS OF ALLOYING ON OXIDATION RESISTANCE OFγ-TiAl BY USING  FIRST PRINCIPLE[J]. 金属学报, 2013, 29(4): 385-390.
[2] . PLASTIC DEFORMATION OF METALLIC MEMBRANE INDUCED BY HYDROGEN PERMEATION[J]. 金属学报, 2007, 43(3): 327-331 .
[3] LIANG Shuhua; XU Lei; FANG Liang; FAN Zhikang. Microstructure and Antibacterial Properties of Cu--Contained Antibacterial Stainless Steel[J]. 金属学报, 2004, 40(3): 309-313 .
[4] LI Tiefan; HU Wusheng; SHEN Jianian(State Key Laboratory of Corrosion Science; Institute of Corrosion and Prolection of Metals; Chinese Academy of Sciences; Shenyang 110015). HIGH TEMPERATURE OXIDATION PERFORMANCE OF SUPERALLOY M41[J]. 金属学报, 1995, 31(24): 527-534.
[5] NING Yuantao;LI Yongnian Kunming Institute of Precious Metals. INTERNAL OXIDATION BEHAVIOR OF Pd-40Ag-1M (M=Zr, Y) ALLOYS[J]. 金属学报, 1989, 25(1): 96-103.
[6] YANG Rui;LI Dong;WAN Xiaojing Institute of Metal Research; Academia Sinica; Shenyang. PHASE BOUNDARY OF α_2 PRECIPITATION IN Ti-Al-La TERNARY SYSTEM[J]. 金属学报, 1988, 24(4): 288-290.
No Suggested Reading articles found!