STRUCTURE AND MAGNETIC PROPERTIES OF Sm_2(Fe_(1-x)Cr_x)17N_(~2.7) MAGNETS
ZHOU Shouzeng;YANG Jun;ZHANG Maocai(University of Science and Technologl. Beijing);LIN Yi; YIN Youxiang;LIN Guobiao(Beijing General institute of Mining and Metallurgy)(Manuscript received 19 May;1993;in revised form 19 August;1993)
Cite this article: 

ZHOU Shouzeng;YANG Jun;ZHANG Maocai(University of Science and Technologl. Beijing);LIN Yi; YIN Youxiang;LIN Guobiao(Beijing General institute of Mining and Metallurgy)(Manuscript received 19 May;1993;in revised form 19 August;1993). STRUCTURE AND MAGNETIC PROPERTIES OF Sm_2(Fe_(1-x)Cr_x)17N_(~2.7) MAGNETS. Acta Metall Sin, 1994, 30(14): 72-76.

Download:  PDF(360KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effect of Cr in substitution for a part of Fe on structure and magnetic properties of Sm_2(Fe_(1-x)Cr_x)_(17)N_(~2.7) alloys powder has been investigated.The structure of the alloys remains the same with an addition of Cr,saying x=0-0.1.With the increase of Cr content,their Curie temperature,anisotropic field.saturation magnetization,average Fe atom moment and average hyperfine field decrease slightly.But their homogeneity may be obviously improved and coercivity increased even up to 1592 kA/m for Sm_2(Fe_0.95Cr_0.05)_17N_(~2.7) powder.
Key words:  SmFeN magnet      nitride magnet      intrinsic magnetic property     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I14/72

1CoeyJMD,SunHong,HurelevDPF.J MagnMagnMater,1991;101:3102刘伟,王群,赵新国,赵彤,张志东,孙校开.金属学报,1993;29:B1263ZhouShouzeng,YangJun,ZhangMaocai,MaDeqing,LiFobiao,WangRun.In:Hi-permLaboratory,ResearchCentreforAdvancedMinoralandMaterialsProcessingeds.,Proc12thIntWorkshoponRareEarthMagnetsandTheirApplcations.TheUniversityofWersternAustralia,Nedland.Australia.1992:444DingJ,McCormichPG,StreetR,SmithPAL,In:Hi-permLaboratory,ResearchCentreforAdvancedMinoralandMaterialsProcessingeds.,Proc7thIntSymponMagneticAnisotropyandCoercivityinRE-TMAlloy,TheUniversityofWesternAustralia,Nedland,Australia,1992:4315KatterM,WeckerJ,KuhrtC,SchultzL.JMagnMagnMater,1992;117:4196YangJun,ZhouShouzeng,ZhangMaocai,LiFobiao,ZhaoJunhua,WangRun.MaterLett,1991;12:2427WalkerLR,WertheimGK,JaccarinaV.PhysRevLett,1961;6:988杨俊.北京科技大学博士学位论文,1992
[1] PAN Hongge; CHEN Yun; CHEN Changpin(Department of Materials Science and Eegineering; Zhejiang University; Hangzhou 310027)YANG Fuming(State Key Laboratory for Magnetism; Institute of Physics; The Chinese Academy of Sciences; Beijing 100080)Correspondent: PAN Hongge; Tel: (0571)7951406 Fax: (0571)7951152. STRUCTURAL CHARACTERIZATION AND INTRINSIC MAGNETIC PROPERLIES OF THE SmFe_(10.7-x)Mo_(1.3)Ga_x COMPOUNDS[J]. 金属学报, 1998, 34(8): 836-840.