Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (19): 323-326    DOI:
Current Issue | Archive | Adv Search |
TRIBOLOGICAL PROPERTIES OF TiN FILM BY ION BEAM ASSISTED DEPOSITION
LIU Hanwei;CHEN Yuanru (Southwest Jiaotong University; Chengdu)ZHANG Xushou (Laboratory of Solid Lubrication; Lanzhou institute of Chemical Physics;Chinese Academy of Sciences; Lanzhou)
Cite this article: 

LIU Hanwei;CHEN Yuanru (Southwest Jiaotong University; Chengdu)ZHANG Xushou (Laboratory of Solid Lubrication; Lanzhou institute of Chemical Physics;Chinese Academy of Sciences; Lanzhou). TRIBOLOGICAL PROPERTIES OF TiN FILM BY ION BEAM ASSISTED DEPOSITION. Acta Metall Sin, 1994, 30(19): 323-326.

Download:  PDF(300KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  XPS, AES and XRD show that the main composition of TiN film prepared by ion beam assisted deposition is TiN with fine grain size and slightly preferential orientation,except predominent TiO_2 on surface of film and a wide mixed region of Ti, Fe, N at interface between film and substrate. The tribological behaviour of the TiN film was tested on a ball/disc frictional device under stepwise loading and lubricating sliding. From P-v diagram, the enlargement of boundary lubrication region has been found. It seems that the existence of TiN film increases the load carrying capacity of substrate of Cr12MoV steel.
Key words:  ion beam assisted deposition      TiN film      sliding friction     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I19/323

1KantRA,SartwellBD.MaterSciEng,1987;90:3572ItoH,YoshidaY,YamajS,MaeyamaY,InaT,MinowaY.NuclInstrtumMethodsPhysRes,1989;B39:1743SmidtFA.IntMaterRev,1990;35:614LiuXianghua,XueBin,ZhengZhihong,ZhouZuyao,ZouShichang.NuclInstrumMethPhysRes,1989;B39:1855刘捍卫.西南交通大学硕士学位论文,1992
[1] Huiying SHI, Chao YANG, Bailing JIANG, Bei HUANG, Di WANG. Influences of Target Peak Current Density on the Microstructure and Mechanical Properties of TiN Films Deposited by Dual Pulsed Power Magnetron Sputtering[J]. 金属学报, 2018, 54(6): 927-934.
[2] YU Li; LIU Jiwen;ZHAO Jie; DAI Shaoxia;JIN Zhujing;WANG Huijun(State Key Laboratory of Corroston and Protection;Institute of Corroston and Protection of Metals; Chinese Academy of Sciences;Shenyang;110015)( Metallurgical College; Mianjing Universily;Tianjin 300400 )(Manuscript received 1995-12-06; in revised form 1996-09-02). EFFECT OF SUBSTRATE TEMPERATURE ON THE PROPERTIES OF ION PLATING TiN FILMS[J]. 金属学报, 1996, 32(12): 1270-1274.
[3] ZHU Hong; LIU Xianghuai; REN Congxin; CHEN Guoliang; ZOU Shichang (Ion Beam Lahoratory Shanghai Institute of Metallurgy; Chinese Academy of Sciences;Shanghai 200050). STRUCTURE AND PROPERTIES OF DIAMOND LIKE CARBON FILMS BY LOW ENERGY ION BEAM ASSISTED DEPOSITION USING A SINGLE ION SOURCE[J]. 金属学报, 1995, 31(15): 139-144.
[4] JIANG Hai; WU Qinglan; TAO kun; LI Hengde(Tsinghua University; Beijing). FORMATION OF IRON NITRIDE FILMS BY ION BEAM ASSISTED DEPOSITION[J]. 金属学报, 1994, 30(18): 273-276.
[5] JIANG Hai;TAO Kun;LI Hengde Tsinghua University. Beijing lecturer;Department of Materials Science and Engineering;Tsinghua University; Beijing 100084. PREPARATION OF B-N FILMS BY ION BEAM ASSISTED DEPOSITION[J]. 金属学报, 1993, 29(4): 77-80.
[6] ZHAO Cheng;PENG Hongrui;LI Shizhi Qingdao Institute of Chemical Technology. PLASMA CHEMICAL VAPOUR DEPOSITION OF Ti-N-C FILMS[J]. 金属学报, 1993, 29(1): 87-92.
[7] LIU Changqing; LI Meishuan; JIN Zhujing; WU Weitao (Corrosion Science Lab.; Institute of Corrosion and Protection of Metals; Academia Sinica. Shenyang 110015). TENSILE AND ADHESIVE STRENGTHS OF FINE TiN FILM ON Ti SUBSTRATE[J]. 金属学报, 1992, 28(9): 91-94.
[8] WANG Xi;YANG Genqing;LIU Xianghuai;ZHENG Zhihong;HUANG Wei;ZHOU Zuyao;ZOU Shichang Ion Beam Laboratory; Shanghai Institute of Metallurgy; Academia Sinica. PREPARATION OF TiN FILMS BY N_2 ASSISTED Xe~+ ION BEAM ENHANCED DEPOSITION AND THEIR MECHANICAL PROPERTIES[J]. 金属学报, 1992, 28(3): 87-91.
[9] WANG Xi;ZHOU Jiankun;CHEN Youshan;LIU Xianghuai;ZOU Shichang Ion Beam Laboratory; Shanghai Institute of Metallurgy; Academia Sinica. COMPUTER SIMULATION OF ION BEAM ENHANCED DEPOSITION OF TiN FILMS[J]. 金属学报, 1991, 27(3): 136-141.
[10] ZHOU Jiankun;LIU Xianghuai;CHEN Youshan;WANG Xi;ZHENG Zhihong;HUANG Wei;ZOU Shichang Shanghai Institute of Metallurgy. Academia Sinica Ion Beam Laboratory;Shanghai Institute of Metallurgy;Academia Sinica; Shanghai 200050. SYNTHESIS OF TiN FILM BY ION BEAM ENHANCED DEPOSITION AND ITS PROPERTIES[J]. 金属学报, 1990, 26(2): 136-141.
[11] LI Shizhi;XU Xiang Qingdao Institute of Chemical Technology; Qingdao; ShandongProfessor;Thin Solid Films Lab.;Qingdao Institute of Chemical Technology;53 Zhengzhou Road; Qingdao; Shandong. PLASMA CHEMICAL VAPOR DEPOSITED TiN FILMS[J]. 金属学报, 1988, 24(3): 229-235.
No Suggested Reading articles found!