Relationship of Inclusions and Rolling Contact Fatigue Life for Ultra-Clean Bearing Steel |
SUN Feilong1, GENG Ke2, YU Feng3, LUO Haiwen1( ) |
1.Metallurgical Department of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083, China 2.Jiangyin Xingcheng Special Steel Works Co. Ltd. , Jiangyin 214400, China 3.Central Iron and Steel Research Institute,Beijing 100081, China |
|
Cite this article:
SUN Feilong, GENG Ke, YU Feng, LUO Haiwen. Relationship of Inclusions and Rolling Contact Fatigue Life for Ultra-Clean Bearing Steel. Acta Metall Sin, 2020, 56(5): 693-703.
|
Abstract The cleanliness of bearing steels produced in China has been greatly improved due to the significant progress in the steelmaking technologies in the past decade, leading to their total oxygen (T.O.) contents lowered to no more than 6×10-6. Under such a high cleanliness, it is then expected that the influence of non-metallic inclusions on fatigue property should be different from the previous knowledge, because both the size and quantity of inclusions are reduced greatly. Therefore, both inclusions and fatigue properties for three ultra-clean GCr15 (100Cr6) bearing steels containing T.O. around 6×10-6, which were manufactured via different industrial production processes, were studied for this purpose. First, inclusions were characterized by ASPEX SEM and then statically analyzed by the statistics of extreme values (SEV) and the generalized Pareto distribution (GPD). Next, their rolling contact fatigue lives (RCF) L10 and L50 were measured by flat washer tests. Only the largest inclusion in each sample is required for predicting the characteristic sizes of maximum inclusion (CSMI) for the three steels using the SEV method. The calculated CSMIs, however, are not consistent with the variation of either L10 or L50, indicating they are not relevant. In contrast, the types of inclusions above threshold (u) size can be classified and their number density of inclusions quantified when the GPD method is employed. In particularly, the CSMIs of different types of inclusions can be determined. In this case, it has been found that the CSMI of TiN inclusion, which is the most dangerous for initiating cracking, is in a good agreement with the low probability rolling fatigue life (L10), suggesting that they are very correlated. This, however, cannot explain the variation of high-probability fatigue life (L50). Instead, the density of total inclusions also played an important role on the L50 of ultra-clean bearing steels in addition to the CSMI of TiN inclusions. This is reasonable because cracking shall be initiated at not only the most dangerous TiN inclusion during the early failure but also some other highly dense inclusions particularly during the late failure. Therefore, it is then concluded that the L10 is much more related to the CSMI of most dangerous TiN inclusion; whilst the L50 is strongly affected by the number density of total inclusions.
|
Received: 10 October 2019
|
|
Fund: National Key Research and Development Program of China(2016YFB0300102);International Science and Technology Cooperation Program of China(2015DFG51950);Fundamental Research Funds for the Central Universities in China(FRF-TP-18-002C2) |
1 |
Tomita Y. Improved fracture toughness of ultrahigh strength steel through control of non-metallic inclusions [J]. J. Mater. Sci., 1993, 28: 853
|
2 |
Tian C, Liu J H, Dong H. Inclusions evaluation and rolling contact fatigue life of high clean bearing steels [J]. Shanghai Met., 2018, 40(4): 1
|
|
田 超, 刘剑辉, 董 瀚. 高洁净轴承钢夹杂物评价与滚动接触疲劳寿命 [J]. 上海金属, 2018, 40(4): 1
|
3 |
Zhang L F, Yang W, Zhang X W, et al. Systematic analysis of non-metallic inclusions in steel [J]. Iron Steel, 2014, 49(2): 1
|
|
张立峰, 杨 文, 张学伟等. 钢中夹杂物的系统分析技术 [J]. 钢铁, 2014, 49(2): 1
|
4 |
Murakami Y. Inclusion rating by statistics of extreme values and its application to fatigue strength prediction and quality control of materials [J]. J. Res. Natl. Inst. Stand. Technol., 1994, 99: 345
|
5 |
Shi G, Atkinson H V, Sellars C M, et al. Application of the generalized Pareto distribution to the estimation of the size of the maximum inclusion in clean steels [J]. Acta Mater., 1999, 47: 1455
|
6 |
Scarf P A, Laycock P J. Applications of extreme value theory in corrosion engineering [J]. J. Res. Natl. Inst. Stand. Technol., 1994, 99: 313
|
7 |
Laycock P J, Scarf P A. Exceedances, extremes, extrapolation and order statistics for pits, pitting and other localized corrosion phenomena [J]. Corros. Sci., 1993, 35: 135
|
8 |
Hetzner D W. Developing ASTM E 2283: Standard practice for extreme value analysis of nonmetallic inclusions in steel and other microstructural features [J]. J. ASTM Int., 2006, 3: 1
|
9 |
Atkinson H V, Shi G. Characterization of inclusions in clean steels: A review including the statistics of extremes methods [J]. Prog. Mater. Sci., 2003, 48: 457
|
10 |
Ma C, Luo H W. Precipitation and evolution behavior of carbide during heat treatments of GCr15 bearing steel [J]. J. Mater. Eng., 2017, 45(6): 97
|
|
马 超, 罗海文. GCr15轴承钢热处理过程中碳化物的析出与演变行为 [J]. 材料工程, 2017, 45(6): 97
|
11 |
Gumbel E J. Statistics of Extremes [M]. New York: Columbia University Press, 1958: 247
|
12 |
Murakami Y, Toriyama T, Coudert E M. Instructions for a new method of inclusion rating and correlations with the fatigue limit [J]. J. Test. Eval., 1994, 22: 318
|
13 |
Beretta S, Murakami Y. Statistical analysis of defects for fatigue strength prediction and quality control of materials [J]. Fatigue Fract. Eng. Mater. Struct., 1998, 21: 1049
|
14 |
Anderson C W, Shi G, Atkinson H V, et al. Interrelationship between statistical methods for estimating the size of the maximum inclusion in clean steels [J]. Acta Mater., 2003, 51: 2331
|
15 |
Anderson C W, Shi G, Atkinson H V, et al. The precision of methods using the statistics of extremes for the estimation of the maximum size of inclusions in clean steels [J]. Acta Mater., 2000, 48: 4235
|
16 |
Shi G, Atkinson H V, Sellars C M, et al. Maximum inclusion size in two clean steels Part 1 Comparison of maximum size estimates by statistics of extremes and generalised Pareto distribution methods [J]. Ironmak. Steelmak., 2000, 27: 355
|
17 |
Shi G, Atkinson H V, Sellars C M, et al. Computer simulation of the estimation of the maximum inclusion size in clean steels by the generalized Pareto distribution method [J]. Acta Mater., 2001, 49: 1813
|
18 |
Zhang J M, Zhang J F, Yang Z G, et al. Estimation of maximum inclusion size and fatigure strength in high strength steel [J]. Acta Metall. Sin., 2004, 40: 846
|
|
张继明, 张建锋, 杨振国等. 高强钢中最大夹杂物的尺寸估计与疲劳强度预测 [J]. 金属学报, 2004, 40: 846
|
19 |
Yates J R, Shi G, Atkinson H V, et al. Fatigue tolerant design of steel components based on the size of large inclusions [J]. Fatigue Fract. Eng. Mater. Struct., 2002, 25: 667
|
20 |
Shi Z Y, Xu H F, Xu D, et al. Characterization of inclusions in GCr15 bearing steel by ASPEX and rotary bending fatigue methods [J]. Iron Steel, 2019, 54(4): 55
|
|
史智越, 徐海峰, 许 达等. 采用ASPEX和旋弯疲劳法表征GCr15轴承钢夹杂物 [J]. 钢铁, 2019, 54(4): 55
|
21 |
Ma C, Luo H W. Inclusion particles of super-clean steel examined by both scanning electron microscope and electrolytic extraction [J]. Metall. Anal., 2017, 37(8): 1
|
|
马 超, 罗海文. 扫描电镜和电解萃取法用于超洁净钢中夹杂物的表征 [J]. 冶金分析, 2017, 37(8): 1
|
22 |
Monnot J, Heritier B, Cogne J Y. Relationship of melting practice, inclusion type, and size with fatigue resistance of bearing steels [A]. Proceedings of Effect of Steel Manufacturing Process on the Quality of Bearing Steels [C]. West Conshohocken, PA: ASTM Int., 1988: 149
|
23 |
Lund T B, Johansson S A, Ölund L J P. Nucleation of fatigue in very low oxygen bearing steels [A]. Proceedings of Bearing Steels: Into the 21st Century [C]. West Conshohocken, PA: ASTM Int., 1998: 124
|
24 |
Fu J, Wang P, Xu J H, et al. Effect and control of minor elements—Oxygen, nitrogen, titanium and calcium in bearing steel [J]. Spec. Steel, 1998, 19(6): 31
|
|
傅 杰, 王 平, 徐君浩等. 轴承钢中微量元素氧-氮-钛-钙的作用与控制 [J]. 特殊钢, 1998, 19(6): 31
|
25 |
University of Science and Technology Beijing. Generalized Pareto method rating software for inclusions in steel GPD. Model V1.0 [CP]. Copyright Registration No. 2018SR904406
|
|
(北京科技大学. 钢中夹杂物的帕累托评级软件. GPDModelV1.0 [CP]. 著作权登记号: 2018SR904406
|
26 |
Shi G, Atkinson H V, Sellars C M, et al. Comparison of extreme value statistics methods for predicting maximum inclusion size in clean steels [J]. Ironmak. Steelmak., 1999, 26: 239
|
27 |
Brooksbank D, Andrews K W. Thermal expansion of some inclusions found in steels and relation to tessellated stresses [J]. J. Iron. Steel. Inst., 1968, 206: 595
|
28 |
Brooksbank D, Andrews K W. Stress fields around inclusions and their relation to mechanical properties [J]. J. Iron. Steel. Inst., 1972, 210: 246
|
29 |
Walker P F F. Improving the reliability of highly loaded rolling bearings: The effect of upstream processing on inclusions [J]. Mater. Sci. Technol., 2014, 30: 385
|
30 |
Hashimoto K, Hiraoka K, Kida K, et al. Effect of sulphide inclusions on rolling contact fatigue life of bearing steels [J]. Mater. Sci. Technol., 2013, 28: 39
|
31 |
Jung I H. Overview of the applications of thermodynamic databases to steelmaking processes [J]. Calphad, 2010, 34: 332
|
32 |
Neishi Y, Makino T, Matsui N, et al. Influence of the inclusion shape on the rolling contact fatigue life of carburized steels [J]. Metall. Mater. Trans., 2013, 44A: 2131
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|