| Liquid-Liquid Phase Separation of Fe-Cu-Pb Alloy and Its Application in Metal Separation and Recycling of Waste Printed Circuit Boards |
Bin CHEN1,2,Jie HE1,2( ),Xiaojun SUN1,2,Jiuzhou ZHAO1,2,Hongxiang JIANG1,Lili ZHANG1,Hongri HAO1 |
1. Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2. School of Materials Science and Engineering, University of Science and Technology of China, Shenyang 110016, China |
|
Cite this article:
Bin CHEN,Jie HE,Xiaojun SUN,Jiuzhou ZHAO,Hongxiang JIANG,Lili ZHANG,Hongri HAO. Liquid-Liquid Phase Separation of Fe-Cu-Pb Alloy and Its Application in Metal Separation and Recycling of Waste Printed Circuit Boards. Acta Metall Sin, 2019, 55(6): 751-761.
|
|
|
Abstract The pyrolysis processing was carried out on the waste printed circuit boards (WPCBs) of mobile phones to dissociate metals from non-metals and obtain mixed metals with Fe, Cu and Pb as main components. Based on the main compositions of Fe, Cu and Pb, the liquid-liquid phase separation behavior of (Fe0.4Cu0.6)100-xPbx ternary alloy has been studied experimentally. The results show that the liquid-liquid phase separation of L→L(Fe)+L(Cu, Pb) may occur during the ternary Fe-Cu-Pb alloy melt cooling in the miscibility gap. After the liquid L(Fe) solidified, the secondary liquid-liquid phase separation L(Cu, Pb)→L(Cu)+L(Pb) takes place in the residual L(Cu, Pb) liquid phase, finally resulting in a three-zone separation structure. On the basis of the behavior of the liquid-liquid phase separation, a self-organized hierarchical separation system has been designed to separate and recycle these mixed metals from WPCBs. The enrichment behavior of the minor components like Cr, Au and Cd in the separation system was explored. The effect of super-gravity level on the metal separation and recycling rates has been discussed. As a result, a new harmless route has been established to recycle metal resources in WPCBs.
|
|
Received: 30 October 2018
|
|
|
| Fund: National Natural Science Foundation of China(Nos.51574216);National Natural Science Foundation of China(51774264);National Natural Science Foundation of China(51374194);Key Project of Innovation Foundation of IMR-CAS(No.SCJJ-2013-ZD-03);Natural Science Foundation of Liaoning Province(No.2015020172) |
| [1] | Jia J, Zhao J Z, Guo J J, et al. Immiscible Alloys and Their Manufacturing Technique [M]. Harbin: Harbin Institure of Technology Press, 2002: 1 | | [1] | (贾 均, 赵九洲, 郭景杰等. 难混溶合金及其制备技术 [M]. 哈尔滨: 哈尔滨工业大学出版社, 2002: 1) | | [2] | He J, Zhao J Z, Li H L, et al. Directional solidification and microstructural refinement of immiscible alloys [J]. Metall. Mater. Trans., 2008, 39A: 1174 | | [3] | He J, Zhao J Z. Microstructure evolution in a rapidly solidified Cu85Fe15 alloy undercooled into the metastable miscibility gap [J]. J. Mater. Sci. Technol., 2005, 21: 759 | | [4] | Bian X F, Zhao X L, Wu Y Q, et al. Effect of magnetic field on binodal temperature in immiscible alloys [J]. J. Appl. Phys., 2013, 114: 131907 | | [5] | Kaban I G, Hoyer W. Characteristics of liquid-liquid immiscibility in Al-Bi-Cu, Al-Bi-Si, and Al-Bi-Sn monotectic alloys: Differential scanning calorimetry, interfacial tension, and density difference measurements [J]. Phys. Rev., 2008, 77B: 125426 | | [6] | Wang T M, Song T, Xu J J, et al. Preparation of homogeneous Al-Bi immiscible alloy by a cooling slope method [J]. Spec. Cast. Nonferrous Alloys, 2008, 28: 578 | | [6] | (王同敏, 宋 涛, 许菁菁等. 冷却斜槽法制备均质Al-Bi系难混溶合金 [J]. 特种铸造及有色合金, 2008, 28: 578) | | [7] | Kolbe M, Gao J R. Liquid phase separation of Co-Cu alloys in the metastable miscibility gap [J]. Mater. Sci. Eng., 2005, A413-414: 509 | | [8] | Cao C D, G?rler G P, Herlach D M, et al. Liquid-liquid phase separation in undercooled Co-Cu alloys [J]. Mater. Sci. Eng., 2002, A325: 503 | | [9] | Wang H P, Wei B. Positive excess volume of liquid Fe-Cu alloys resulting from liquid structure change [J]. Phys. Lett., 2010, 374A: 4787 | | [10] | Gao J, Wang Y P, Zhou Z M, et al. Phase separation in undercooled Cu-Cr melts [J]. Mater. Sci. Eng., 2007, A449-451: 654 | | [11] | Li J Q, Ma B Q, Min S, et al. Effect of Ce addition on macroscopic core-shell structure of Cu-Sn-Bi immiscible alloy [J]. Mater. Lett., 2010, 64: 814 | | [12] | Wang C P, Liu X J, Ohnuma I, et al. Formation of immiscible alloy powders with egg-type microstructure [J]. Science, 2002, 297: 990 | | [13] | Wang H P, Wei B B. Understanding atomic-scale phase separation of liquid Fe-Cu alloy [J]. Chin. Sci. Bull., 2011, 56: 3416 | | [14] | He J, Zhao J Z, Ratke L. Solidification microstructure and dynamics of metastable phase transformation in undercooled liquid Cu-Fe alloys [J]. Acta Mater., 2006, 54: 1749 | | [15] | Jiang H X, Sun Q, Zhao J Z. Effect mechanism of a direct current on the solidification of immiscible alloys [J]. Chin. Phys. Lett., 2012, 29: 088104 | | [16] | He J, Li H Q, Zhao J J, et al. Al-based metallic glass composites containing fcc Pb-rich crystalline spheres [J]. App. Phys. Lett., 2008, 93: 131907 | | [17] | He J, Li H Q, Yang B J, et al. Liquid phase separation and microstructure characterization in a designed Al-based amorphous matrix composite with spherical crystalline particles [J]. J. Alloys Compd., 2010, 489: 535 | | [18] | Ziewiec K, K?dzierski Z, Zielińska-Lipiec A, et al. Formation, properties and microstructure of amorphous/crystalline composite Ag20Cu30Ti50 alloy using miscibility gap [J]. J. Alloys Compd., 2009, 482: 114 | | [19] | Kündig A A, Ohnuma M, Ohkubo T, et al. Glass formation and phase separation in the Ag-Cu-Zr system [J]. Scr. Mater., 2006, 55: 449 | | [20] | He J, Mattern N, Tan J, et al. A bridge from monotectic alloys to liquid-phase-separated bulk metallic glasses: Design, microstructure and phase evolution [J]. Acta Mater., 2013, 61: 2102 | | [21] | Kim M U, Ahn J P, Seok H K, et al. Application of spinodal decomposition to produce metallic glass matrix composite with simultaneous improvement of strength and plasticity [J]. Met. Mater. Int., 2009, 15: 193 | | [22] | Eckert J, Das J, Kim K B, et al. High strength ductile Cu-base metallic glass [J]. Intermetallics, 2006, 14: 876 | | [23] | He J, Wang Z Y, Hao H R, et al. Method for efficient separation and recycling of precious metals in waste circuit board [P]. Chin Pat, CN 104328281 B, 2016 | | [23] | (何 杰, 王中原, 郝红日等. 一种高效分离与回收废弃线路板中贵金属的方法 [P]. 中国专利, CN 104328281 B, 2016) | | [24] | He J, Wang Z Y, Hao H R, et al. Self-assembly separation and resource recycling method for multi-metal components in electronic waste [P]. Chin Pat, CN 104313332 B, 2016 | | [24] | (何 杰, 王中原, 郝红日等. 电子垃圾中多金属组分自组装分离与资源化回收的方法 [P]. 中国专利, CN 104313332 B, 2016) | | [25] | Chen B, He J, Xi Y Y, et al. Liquid-liquid hierarchical separation and metal recycling of waste printed circuit boards [J]. J. Hazard. Mater., 2019, 364: 388 | | [26] | Chen B, He J, Zhao J Z. Phase separation of Fe-Cu-Pb alloy and recycling of mixed metals in waste printed circuit boards [J]. Mater. Sci. Forum, 2019, 944: 1265 | | [27] | Yamaguchi K, Takeda Y. Copper enrichment of scrap by phase separation in liquid Fe-Cu-C system [J]. Shigen Sozai, 1997, 113: 1110 | | [27] | (山口 勉功, 武田 要一. Fe-Cu-C系2液相分離による低品位銅スクラップからの銅の濃縮 [J]. 資源と素材, 1997, 113: 1110) | | [28] | State Environmental Protection Administration. Administrative measures on the prevention and control of environmental pollution by electronic waste [J]. Recycl. Resour. Circul. Econ., 2007, (6): 1 | | [28] | (国家环境保护总局. 电子废物污染环境防治管理办法 [J]. 再生资源与循环经济, 2007, (6): 1) | | [29] | Hadi P, Xu M, Lin C S K, et al. Waste printed circuit board recycling techniques and product utilization [J]. J. Hazard. Mater., 2015, 283: 234 | | [30] | Ministry of Environmental Protection of the People's Republic of China. List of national hazardous waste [EB/OL]. (2016-06-14). http://www.mee.gov.cn/gkml/hbb/bl/201606/t20160621_354852.htm | | [30] | (中华人民共和国环境保护部. 国家危险废物名录 [EB/OL]. (2016-06-14). http://www.mee.gov.cn/gkml/hbb/bl/201606/t20160621_354852.htm) | | [31] | Huang K, Guo J, Xu Z M. Recycling of waste printed circuit boards: A review of current technologies and treatment status in China [J]. J. Hazard. Mater., 2009, 164: 399 | | [32] | Li J, Gao B, Xu Z M. New technology for separating resin powder and fiberglass powder from fiberglass-resin powder of waste printed circuit boards [J]. Environ. Sci. Technol., 2014, 48: 5171 | | [33] | Marra A, Cesaro A, Belgiorno V. Separation efficiency of valuable and critical metals in WEEE mechanical treatments [J]. J. Clean. Prod., 2018, 186: 490 | | [34] | Marques A C, Marrero J M C, de Fraga Malfatti C. A review of the recycling of non-metallic fractions of printed circuit boards [J]. SpringerPlus, 2013, 2: 521 | | [35] | Long L S, Sun S Y, Zhong S, et al. Using vacuum pyrolysis and mechanical processing for recycling waste printed circuit boards [J]. J. Hazard. Mater., 2010, 177: 626 | | [36] | Zhan L, Xu Z M. Separating criterion of Pb, Cd, Bi and Zn from metallic particles of crushed electronic wastes by vacuum evaporation [J]. Sep. Sci. Technol., 2012, 47: 913 | | [37] | Guo X Y, Liu J X. Optimization of low-temperature alkaline smelting process of crushed metal enrichment originated from waste printed circuit boards [J]. J. Cen. South Univ., 2015, 22: 1643 | | [38] | Zhou Y H, Qiu K Q. A new technology for recycling materials from waste printed circuit boards [J]. J. Hazard. Mater., 2010, 175: 823 | | [39] | Lin K H, Chiang H L. Liquid oil and residual characteristics of printed circuit board recycle by pyrolysis [J]. J. Hazard. Mater., 2014, 271: 258 | | [40] | Hall W J, Williams P T. Separation and recovery of materials from scrap printed circuit boards [J]. Resour., Conserv. Recycl., 2007, 51: 691 | | [41] | Takeuchi A, Inoue A. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element [J]. Mater. Trans., 2005, 46: 2817 | | [42] | Yan N, Wang W L, Luo S B, et al. Correlated process of phase separation and microstructure evolution of ternary Co-Cu-Pb alloy [J]. Appl. Phys., 2013, 113A: 763 | | [43] | Yan N, Wang W L, Wei B. Complex phase separation of ternary Co-Cu-Pb alloy under containerless processing condition [J]. J. Alloys Compd., 2013, 558: 109 | | [44] | Onderka B, Jendrzejczyk-Handzlik D, Fitzner K. Thermodynamic properties and phase equilibria in the ternary Cu-Pb-Fe system [J]. Arch. Metall. Mater., 2013, 58: 541 | | [45] | He J, Mattern N, Kaban I, et al. Enhancement of glass-forming ability and mechanical behavior of zirconium-lanthanide two-phase bulk metallic glasses [J]. J. Alloys Compd., 2015, 618: 795 | | [46] | Wang Z Y, He J, Yang B J, et al. Effect of addition of elements on two-glass-forming ability of Zr-Ce-Co-Cu immiscible alloys [J]. Mater. Sci. Technol., 2017, 33: 1926 | | [47] | Wang Z Y, He J, Yang B J, et al. Liquid-liquid phase separation and formation of two glassy phases in Zr-Ce-Co-Cu immiscible alloys [J]. Acta Metall. Sin., 2016, 52: 1379 | | [47] | (王中原, 何 杰, 杨柏俊等. Zr-Ce-Co-Cu难混溶合金的液-液相分离和双非晶相形成 [J]. 金属学报, 2016, 52: 1379) | | [48] | Lu X, Nakajima K, Sakanakura H, et al. Thermodynamic estimation of minor element distribution between immiscible liquids in Fe-Cu-based metal phase generated in melting treatment of municipal solid wastes [J]. Waste Manag., 2012, 32: 1148 | | [49] | Yang Y H, Song B, Song G Y, et al. Enriching and separating primary copper impurity from Pb-3 mass pct Cu melt by super-gravity technology [J]. Metall. Mater. Trans., 2016, 47B: 2714 | | [50] | Ratke L, Voorhees P W. Growth and Coarsening: Ostwald Ripening in Material Processing [M]. Berlin, Heidelberg: Springer, 2002: 242 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|