| [1] Rohrer G S. J Mater Sci, 2011; 46: 5811 [2] Gleiter H, Chalmers B. Progress Mater Sci, 1972; 14: 1 [3] Brandon D G. Acta Metall, 1966; 14: 1479 [4] Randle V, Owen G. Acta Mater, 2006; 54: 1777 [5] Kobayashi S, Nakamura M, Tsurekawa S, Watanabe T. J Mater Sci, 2011; 46: 4254 [6] Watanabe T. J Mater Sci, 2011; 46: 4095 [7] Mitchell R J, Li H Y, Huang Z W. J Mater Process Technol, 2009; 209: 1011 [8] Safari J, Nategh S. J Mater Process Technol, 2006; 176: 240 [9] Larson J M, Floreen S. Metall Trans, 1977; 8A: 51 [10] Lizuka H, Tanaka M. J Mater Sci, 1990; 25: 3785 [11] Yeh A C, Lu K W, Kuo C M, Bor H Y, Wei C N. Mater Sci Eng, 2011; A530: 525 [12] Hong H U. Metall Mater Trans, 2012; 43A: 173 [13] Koul A K, Thamburaj R. Metall Trans, 1985; 16A: 17 [14] Kim K J, Hong H U, Nam S W. Mater Chem Phys, 2011; 126: 480 [15] Miyagawa O, Yamamoto M, Kobayashi M. In: Muzyka D R, Couts W H, Walelewski G E, Kear B H, Stroup J P, Dreshfield R L, Morrow H eds., Superalloys 1976, Warrendale PA: TMS, 1976: 245 [16] Konopleva E V, Mcqueen H J, Evangelista E. Mater Character, 1995; 34: 251 [17] Koul A K, Gessinger G H. Acta Metall, 1983; 31: 1601 [18] Wu Q, Song H, Swindeman R W, Shingledecker J P, Vasudevan V K. Metall Mater Trans, 2008; 39A: 2569 [19] Huang Y, Wang L, Liu Y, Fu S, Wu J, Yan P. Trans Nonferrous Met Soc China, 2011; 21: 2199 [20] Qin X Z, Guo J T, Yuan C, Chen C L, Ye H Q. Metall Mater Trans, 2007; 38A: 3014 [21] Koul A K, Castillo R. Metall Trans, 1988; 19A: 2049 [22] Iwashita C H, Wei R P. Acta Mater, 2000; 48: 3145 [23] Rylands L M, Wilkes D M J, Rainforth W M, Jones H. J Mater Sci, 1994; 29: 1895 [24] Ardell A J. Acta Metall, 1972; 20: 601 [25] Christian J W. The Theory of Transformations in Metals and Alloys. 2nd Ed., Kidlington: Pregamon, 2002: 529 [26] Zeng Q, Wen X, Zhai T. Mater Sci Eng, 2008; A476: 290 [27] Cahn J W. Acta Metall, 1956; 4: 449 [28] Choi B G, Kim I S, Kim D H, Jo C Y. Mater Sci Eng, 2008; A478: 329 [29] Qin X Z, Guo J T, Yuan C, Hou J S, Zhou L Z, Ye H Q. Mater Sci Eng, 2012; A543: 121 [30] Liu W C, Morris J G. Metall Mater Trans, 2005; 36A: 2829 [31] Cahn J W. Acta Metall, 1957; 5: 169 |