MEASUREMENT OF THE DIFFUSIVITY OF OXYGEN IN HIGH-TEMPERATURE LIQUID SILVER BY ELECTROCHEMICAL METHOD
GAO Yunming1); SONG Jianxin1); ZHANG Yeqin1); GUO Xingmin2)
1) Key Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education; Wuhan University of Science and Technology; Wuhan 430081 2) Metallurgical and Ecological Engineering School; University of Science and Technology Beijing; Beijing 100083
Cite this article: 

GAO Yunming SONG Jianxin ZHANG Yeqin GUO Xingmin. MEASUREMENT OF THE DIFFUSIVITY OF OXYGEN IN HIGH-TEMPERATURE LIQUID SILVER BY ELECTROCHEMICAL METHOD. Acta Metall Sin, 2010, 46(3): 277-281.

Download:  PDF(825KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The diffusivity of oxygen in liquid silver in the temperature range of 1473 to 1773 K were determined by potentiostatic methods employing the following zirconia base solid electrolyte cell arrangement of cylindrical geometry: (+)Pt ︳air ︳ZrO2(MgO)︳[O]Ag(l) ︳Ir(-). The diffusivity of oxygen in liquid silver was calculated from the change of the external current with time by applying a preselected voltage on the electrochemical cell. The relation between oxygen diffusivity and temperature was given: Do=(1.11+-0.04)*10^(-3)exp[(-25573+-1718)/RT]cm2s-1 (1473~1773K) The present experimental results were in close agreement with those extrapolated from the predecessors’ data at low temperature. The diffusivity of oxygen in liquid silver at 1773K was found to be (1.96+-0.28)*10^(-4) cm2s-1.

Key words:  liquid silver      oxygen diffusivity      solid electrolyte      electrochemical cell      metallurgy with controlled oxygen flow     
Received:  04 September 2009     
Fund: 

Supported by National High Technology Research and Development Program of China No.2006AA06Z125)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2009.00579     OR     https://www.ams.org.cn/EN/Y2010/V46/I3/277

[1] Chou K C, Gao Y M, Guo X M, Lu X G, Xu K D. Proc 10th Japan–China Symposium on Science and Technology of Iron and Steel. Tokyo: The Iron and Steel Institute of Japan, 2004: 162
[2] Gao Y M, Guo X M, Chou K C. J Chongqing Univ, 2006; 29(8): 123
(高运明, 郭兴敏, 周国治. 重庆大学学报, 2006; 29(8): 123)
[3] Pal Uday B. JOM, 2008; 60: 43
[4] Shah I D, Parlee N A D. Trans TMS–AIME, 1967; 239: 763
[5] Mizikar E A, Grace R E, Parlee N A D. Trans ASM, 1963; 56: 101
[6] Masson C R, Whiteway S G. Can Metall Q, 1967; 6: 199
[7] Sano N, Honma S, Matsushita Y. Metall Trans, 1970; 1: 301
[8] Otsuka S, Kozuka Z. Trans JIM, 1974; 15: 32
[9] Oberg K E, Friedman L M, Boorstein W M, Rapp R A. Metall Trans, 1973; 4: 61
[10] Rickert H, El Miligy A A. Z Metallk, 1968; 59: 635
[11] Otsuka S, Katayama I, Kozuka Z. Trans JIM, 1971; 12: 442
[12] Ramanarayanan T A, Rapp R A. Metall Trans, 1972; 3: 3239
[13] Bernard G, Lupis C H P. Metall Trans, 1971; 2: 555
[14] He C X. Phase Diagrams and Structural Parameter of Alloys and Compound of Noble Metal. Beijing: Metallurgical Industry Press, 2007: 24, 26
(何纯孝. 贵金属合金相图及化合物结构参数.北京: 冶金工业出版社, 2007: 24, 26)

[1] GAO Yunming, HE Lin, QIN Qingwei, LI Guangqiang. ZrO2 Solid Electrolyte Aided Investigation on Electrodeposition in Na3AlF6-SiO2 Melt[J]. 金属学报, 2022, 58(10): 1292-1304.
[2] YU Jingkun; LIU Tao; CHEN Min. EXPERIMENTAL RESEARCH ON SULPHUR CONCENTRATION CELL WITH MgS+1.5%ZrS2 SOLID ELECTROLYTE[J]. 金属学报, 2005, 41(12): 1285-1288 .
[3] LI Fushen; JIN Congjin; LU Xionggang; ZHOU Guozhi; ZHU Lixin; HU Xiaojun; LI Zeya; WANG Feng; SHEN Qiang. OXYGEN RERISING PHENOMENON DURING DEOXIDATION WITH SOLID ELECTROLYTE DEOXIDATION UNITS IN STEEL MELTS[J]. 金属学报, 2004, 40(7): 673-676 .
[4] CHEN Wei; WANG Changzhen; LIU Liang(Northeastern University; Shenyang110006)(Manuscript received 1994-02-10; in revised form 1994-11-08). A STUDY ON SENSOR-PROCEDURE FOR MEASURING HYDROGEN ACTIVITY IN MOLTEN Al ALLOY[J]. 金属学报, 1995, 31(19): 305-310.
[5] ZOU Kaiyun; WANG Changzhen; (Faculty of Metallurgical Phisical Chemislry; Northeastern Universily. Shenyang 110006) ZHAO Nairen (Northeastern University; Shenyang 110006). LANTHANUM SENSOR AND ACTIVITY OF LANTHANUM IN CARBON SATURATED IRON[J]. 金属学报, 1995, 31(17): 195-199.
[6] XIE Gang; SONG Ning(Kunming Institute of Technology). DETERMINATION OF ACTIVITIES IN MELTED NaF-AlF_3 SYSTEM[J]. 金属学报, 1994, 30(17): 199-203.
[7] ZHANG Qianxian University of science and Technology Beijing. DETERMINATION OF ACTIVITY OF Al IN SOLID Cu-Al ALLOYS[J]. 金属学报, 1989, 25(2): 149-151.
No Suggested Reading articles found!