| INFLUENCE OF Cl$^{-}$ CONCENTRATION ON CREVICE CORROSION OF X70 PIPELINE STEEL |
| SONG Yiquan1; DU Cuiwei2; ZHANG Xin2; LI Xiaogang2;3 |
1) School of Material and Metallurgy; Inner Mongolia University of Science and Technology; Baotou 014010
2) The Key Lab of Corrosion; Erosion and Surface Technology of Beijing; Corrosion and Protection Center of University of Science and Technology Beijing; Beijing 100083
3) State Key Laboratory of Corrosion and Protection; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015 |
|
Cite this article:
SONG Yiquan DU Cuiwei ZHANG Xin LI Xiaogang. INFLUENCE OF Cl$^{-}$ CONCENTRATION ON CREVICE CORROSION OF X70 PIPELINE STEEL. Acta Metall Sin, 2009, 45(9): 1130-1134.
|
|
|
Abstract The influence of Cl- concentration in corrosion medium to crevice corrosion of X70 pipeline steel was investigated by wedge-type crevice model. The experimental results show that under natural corrosion condition, as the crevice opening thickness is 0.15 mm and the test periodic is 120 h,\linebreak with increase of the Cl- concentration (cmCl-) in corrosion medium outside the crevice the Cl- concentration (cmCl-) in the crevice solution from the opening to the bottom gradually increases, the pH value in the crevice solution and the electrode potential of X70 steel samples from the opening to the bottom in the crevice gradually decrease, which indicated that crevice corrosion tendency of X70 steel increases with increase of the Cl- concentration (cmCl-) in corrosion medium outside the crevice.
|
|
Received: 11 May 2009
|
|
|
| Fund: Supported by National Natural Science Foundation of China (Nos.50301003 and 50461004) and “Spring Sunshine Plan” Research Project of Ministry of Education of China (No.Z2004-2-15022) |
| [1] Toncre A C. Mater Performance, 1984; 23: 22
[2] Gan F, Sun Z W, Sabde G, Chin D T. Corrosion, 1994; 50: 804
[3] Han X P. Nat Gas Ind, 2001; 21(1): 108
(韩兴平. 天然气工业, 2001; 21(1): 108)
[4] Peterson M H, Lennox T J. Corrosion, 1973; 29: 406
[5] Toncre A C, Ahmad N. Mater Performance, 1980; 19: 39
[6] Turnball A, May A T. Mater Performance, 1983; 22: 34
[7] Fessle R R, Markworth A J, Parkins R N. Corrosion, 1983; 39: 20
[8] Perdomo J J, Song I. Corros Sci, 2000; 42: 1389
[9] Li Z F, Gan F X, Mao X H. Corros Sci, 2002; 44: 689
[10] Margarit I C P, Mattos O R. Electrochim Acta, 1998; 44: 363
[11] Li Z F, Mao X H, Gan F X. J Chin Soc Corros Protect, 2000; 20: 129
(李正奉, 毛旭辉, 甘复兴. 中国腐蚀与防护学报, 2000; 20: 129)
[12] Zhu R Z. Corrosion of Metals. Beijing: Metallurgical Industry
Press, 1993: 111
(朱日彰. 金属腐蚀学. 北京: 冶金工业出版社, 1993: 111)
[13] Chang H Y, Park Y S, Hwang W S. Mater Process Technol,
2000; 10: 206 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|