HIGH TEMPERATURE WEAR BEHAVIOR OF NiAl--Cr(Mo)--Ho--Hf EUTECTIC ALLOY
WANG Zhensheng1;2;GUO Jianting1;ZHOU Lanzhang1;SHENG Liyuan1;HU Zhuangqi1
1 Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016
2 School of Electromechanical Engineering; Hunan University of Science and Technology; Xiangtan 411201
Cite this article: 

WANG Zhensheng GUO Jianting ZHOU Lanzhang SHENG Liyuan HU Zhuangqi. HIGH TEMPERATURE WEAR BEHAVIOR OF NiAl--Cr(Mo)--Ho--Hf EUTECTIC ALLOY. Acta Metall Sin, 2009, 45(3): 297-301.

Download:  PDF(990KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The wear behaviors of NiAl--28Cr--5.6Mo--0.25Ho--0.15Hf eutectic alloy against SiC ceramic under dry sliding from 600 to 1000 ℃ were investigated on a pin--on--disc test rig. The results show that the eutectic alloy exhibits excellent self--lubricating properties in the temperature range of 700---900 ℃, which is attributed to the formation of 1---3 μm thick glass--ceramic lubricant film. During wear testing the lubricant film was partially transferred to the SiC counterface, which avoided the direct tribo--contact between the alloy and SiC ceramic. At temperatures above 900 ℃ or below 700 ℃ the friction coefficient and wear rate are higher, owing to the adhesion between matrix and film weakening or no film forming.

Key words:  NiAl--Cr(Mo)--Ho--Hf eutectic alloy      SiC ceramic      friction and wear behavior      self--lubricating      glass--ceramic film     
Received:  04 August 2008     
ZTFLH: 

TH117.1

 
  TG146.1

 

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I3/297

[1] Guo J T. Ordered Intermetallic Compound NiAl Alloy. Beijing: Science Press, 2003: 75
(郭建亭. 有序金属间化合物镍铝合金. 北京: 科学出版社, 2003: 75)

[2] Johnson B J, Kennedy F E, Baker I. Wear, 1996; 192: 241
[3] Hawk J A, Alman D E. Mater Sci Eng, 1997; A239–240: 899
[4] Hawk J A, Alman D E. Wear, 1999; 225–229: 544
[5] Wang Z S, Zhou L Z, Guo J T, Sheng L Y, Hu Z Q. Tribology, 2008; 28: 497
(王振生, 周兰章, 郭建亭, 盛立远, 胡壮麒. 摩擦学学报, 2008; 28: 497)

[6] Jiang X X, Li S Z, Li S. Corrosive Wear of Metals. Beijing: Chemical Industry Press, 2003: 78
(姜晓霞, 李诗卓, 李曙. 金属的腐蚀磨损. 北京: 化学工业出版社, 2003: 78)

[7] Kingery W D, Bowen H K, Uhlmann D R, Translated by
Zhuang B Q. Ceramic Introduction. Beijing: China Architecture and Building Press, 1987: 368
(Kingery W D, Bowen H K, Uhlmann D R, 著; 庄炳群, 译. 陶瓷导论. 北京: 中国建筑工业出版社, 1987: 368)

[8] Liu R T, Li X B, Cheng S H. Chin J Nonferrous Met, 2003; 13: 469
(刘如铁, 李溪滨, 程时和. 中国有色金属学报, 2003; 13: 469)

[9] Stott F H, Glascott J, Wood G C. Wear, 1985; 101: 311
[10] Jiang J R, Stott F H, Stack M M. Wear, 1994; 176: 185
[11] Ouyang J H, Sasaki S, Murakami T, Umeda K. Ceram Int, 2005; 31: 543

No related articles found!
No Suggested Reading articles found!