Effect of electroslag remelting on tensile properties and fracture mechanism of TiC reinforced 2Cr13 stainless steel
;;;
东南大学 材料科学与工程系
Cite this article: 

;. Effect of electroslag remelting on tensile properties and fracture mechanism of TiC reinforced 2Cr13 stainless steel. Acta Metall Sin, 2008, 44(6): 745-750 .

Download:  PDF(11718KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Tensile properties of the matrix 2Cr13, TiC reinforced 2Cr13 steels prepared by in-situ reaction and electroslag remelting have been investigated. Experimental results show that introduction of TiC particles to 2Cr13 steel result in significant increase of tensile strength and remarkable decrease of ductility as well as impact toughness of the steel. The mechanism responsible for the fracture of the TiC reinforced 2Cr13 steel without electroslag remelting is mainly the failure of TiC particles due to the large size and distribution ununiformity of the particles in its microstructure. The particles in the steel processed by electroslag remelting are fine and their distribution is uniform. During tests cracking of the particles in the electroslag remelted steel is not easy to occur and the mechanism responsible for the fracture of its specimens is basically the failure of interfaces between particles and matrix.
Key words:       
Received:  27 August 2007     
ZTFLH:  TG111.91  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I6/745

[1]Warren R.Mater Sci,1980;15:2489
[2]Dufour L C.Surface and Interface of Ceramic/Metal Ma- terials.London:Kluwer Academic Publisher,1989:393
[3]Chen J,Wang Z F,Bian J H,Wang X M.Acta Metall Sin, 2001;37:207 (陈俊,王执福,边建华,王晓明.金属学报,2001;37:207)
[4]Pagounis E,Lindroos V K.Mater Sci Eng,1998;A246: 221
[5]Wu Q L,Sun Y S,Yang C D.Mater Trans,2006;47:2393
[6]Wu R J.Acta Metall Sin,1997;33:79 (吴人杰.金属学报,1997,33:79)
[7]Wang Q P,Yao M,Chen G.J Jiangsu Univ,2003;24:57 (王庆平,姚明,陈刚.江苏大学学报(自然科学版),2003;24:57)
[8]Sun Y S,Huang H B,He H Y,Cai L,Xue F,Mei J P, Wang S Q.China Pat ZL99114272.1,2002 (孙扬善,黄海波,何华英,蔡磊,薛烽,梅建平,王仕勤.中国专利ZL99114272.1,2002)
[9]Lucia F,Dunitrescu S,Hillert M.ISIJ Int,1999;39(1):84
[10]Hernandez-Morales B,Mitchell A.lronmak Steelmak, 1999;26:423
[11]Ma J G,Huang M P,You X Q,Ren H,Si T Z.Spec Cast Nonferrous Alloys,2005;25:16 (马建国,黄曼平,尤显卿,任吴,斯庭智.特种铸造及有色合金.2005;25:16)
[12]Singh P M,Lewandowski J J.Metall Trans,1993;24A: 2531
[13]Corbin S F,Wilkinson D S.Acta Metall Mater,1994;42: 1329
[14]Clyne T W,Withers P J(eds.),Yu Y N,Fang Z G(trans.). Metal Matrix Composite.Beijing:Metallurgical Industry Press,1996:26 (克莱因T W,威瑟斯P J著,余永宁,房志刚译.金属基复合材料导论.北京:冶金工业出版社,1996:26)
[15]Sun J R.PhD Thesis,Southeast University,Nanjing,2001 (孙建荣.东南大学博士学位论文,南京,2001)
[16]Wang L,Niinomi M,Takahashi S,Hagiwara M,Emura S, Kawabei Y,Kim S J.Mater Sci Eng,1999;A263:319
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!