| MOLECULAR DYNAMICS SIMULATION OF STRENGTHENING MECHANISM OF Cu/Ni MULTILAYERS |
| CHENG Dong1; YAN Zhijun1; YAN Li2 |
1.Marine Engineering College; Dalian Maritime University
2.Institute of Materials and Technology; Dalian Maritime University |
|
Cite this article:
CHENG Dong YAN Zhijun YAN Li. MOLECULAR DYNAMICS SIMULATION OF STRENGTHENING MECHANISM OF Cu/Ni MULTILAYERS. Acta Metall Sin, 2008, 44(12): 1461-1464.
|
|
|
Abstract The movement of glide dislocations in Cu/Ni films during nano indentation and friction was simulated by using 3D and 2D molecular dynamics methods respectively, and the interactions between interface and glide dislocations were analyzed. The results show that the repulsive force produced by the misfit dislocation network at the interface prevents the glide dislocations accessing or passing through the interfaces; the image force arising from the modulus difference across an interface confines the glide dislocations to move within Cu individual layer. Both of the above forces can be used to explain the strengthening mechanism of Cu/Ni multilayers.
|
|
Received: 01 February 2008
|
|
|
[1]Misra A,Kung H,Embury J D.Scr Mater,2004;50:707 [2]Was G S,Foecke T.Thin Solid Films,1996;286:1 [3]Koehler J S.Phys Rev,1970;2B:547 [4]Embury J D,Hirth J P.Acta Metall Mater,1994;42:2051 [5]Hall E O.Proc Phys Soc,1952;64B:747 [6]Petch N J.Iron Steel Inst,1953;174:25 [7]Zhou X W,Wadley H N G,Johnson R A.Acta Mater, 2001;49:4005 [8]Halle J M.Molecular Dynamics Simulation:Elementary Methods.New York:John Wiley,1992:159 [9]Parrinello M,Rahman A.J Appl Phys,1981;52:7180 [10]Cheng D,Yah Z J,Yah L.Thin Solid Films,2007;515: 3698 [11]Knap J,Ortiz M.Phys Rev Lett,2003;90:226102-1 [12]Yu Y N.Principles of Metallography.Beijing:Metallur- gical Industry Press,2003:299,310 (余永宁.金属学原理.北京:冶金工业出版社,2003:299,310) [13]Cheng D,Yah Z J,Yan L.Acta Metall Sin,2006;42:118 (程东,严志军,严立.金属学报,2006;42:118) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|