| ANALYSIS OF LIQUID FRICTION MECHANISM FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED |
| Xiang-Ning MENG;Miao-Yong ZHU |
| 东北大学 |
|
Cite this article:
Xiang-Ning MENG; Miao-Yong ZHU. ANALYSIS OF LIQUID FRICTION MECHANISM FOR SLAB CONTINUOUS CASTING MOLD WITH HIGH CASTING SPEED. Acta Metall Sin, 2008, 44(10): 1193-1197 .
|
|
|
Abstract On the basis of laws of momentum and mass conservation of liquid flux, a mathematical model to represent the liquid friction force in meniscus under non-sinusoidal oscillation was established, and a new liquid friction mechanism was proposed by solving extremum equations of liquid friction force as 2.0 m•min-1 casting speed. The results show that liquid friction force was mainly influenced by the shape of flux channel, depth of molten flux pool and relative motion between oscillating mold and strand and varies with oscillation waveform. Maximum liquid friction force occurs nearby the moment of oscillation velocity equal to casting speed under an ideal state. Surface cracks formed in the positive strip time adjacent to negative strip time, and healed during the negative strip time.
|
|
Received: 24 March 2008
|
|
|
[1]Yao M,Wang W H,Wei S L,Yin H B,Fang D C.J Dalian Univ Technol,2002;42:195 (姚曼,王文华,魏树立,尹合壁,方大成.大连理工大学学报,2002:42:195) [2]Li X K,Zhang D M.Continuous Casting Mold Oscillation Technology.Beijing:Metallurgical Industry Press,2000: 30 (李宪奎,张德明.连铸结晶器振动技术.北京:冶金工业出版社,2000:30) [3]Hwang Y S,Cha P R,Nam H S,Moon K H,Yoon J K. ISIJ Int,1997;37:659 [4]Zhang J M,Zhang L,Wang X H,Wang L F.Acta Metall Sin,2003;39:1285 (张炯明,张立,王新华,王立峰.金属学报,2003;39:1285) [5]Okazawa K,Kajitani T,Yamada W,Yamamura H.ISIJ Int,2006;46:226 [6]Meng X N,Zhu M Y,Liu X D,Cheng N L,Jiang Z K. Acta Metall Sin,2007;43:205 (孟祥宁,朱苗勇,刘旭东,程乃良,江中块.金属学报,2007;43:205) [7]Takeuchi E,Brimacombe J K.Metall Trans,1984;15B: 493 [8]Suzuki M,Mizukami H,Kitagawa T,Kawakami K,Uchida S,Komatsu Y.ISIJ Int,1991;31:254 [9]Mizukami H,Kawakami K,Kitagawa T,Suzuki M,Uchida S,Komatsu Y.Tetsu Hagané,1986;72:1862 (水上秀昭,川上公成,北川融,铃木干雄,内田繁孝,小松喜美.铁と钢,1986;72:1862) [10]Zhang H B,Wang H Z.Iron Steel,1995;30(11):17 (张洪波,王海之.钢铁,1995;30(11):17) [11]Kajitani T,Okazawa K,Yamada W,Yamamura H.ISIJ Int,2006;46:1432 [12]Meng Y,Thomas B G.ISIJ Int,2006;46:660 [13]Meng X N,Zhu M Y.Chin Mech Eng,2007;18:1779 (孟祥宁,朱苗勇.中国机械工程,2007;18:1779) [14]Sumi I,Shimizu H,Nishioka S,Nakada M,Murakami K, Suzuki M.ISIJ Int,2003;43:807 [15]Meng X N,Zhu M Y,Cheng N L.Acta Metall Sin,2007; 43:839 (孟祥宁,朱苗勇,程乃良金属学报,2007;43:839) [16]Yukio N,Youichi F.ISIJ Int,1984;24:1262 [17]Gan Y,Chen D L,Yang W G.Iron Steel,1999;34(4):16 (干勇,陈栋梁,杨文改.钢铁,1999;34(4):16) [18]Zang X Y,Wang X D,Ma Y,Yao M,Zhang L.Iron Steel, 2007;42(10):39 (臧欣阳,王旭东,马勇,姚曼,张立.钢铁,2007;42(10):39) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|