| The influence of hydrogen on ultra-high cycle fatigue properties of high strength spring steel 50CrV4 |
| Yongde LI;shou xin LI;;;;; |
| 沈阳中科院金属研究所疲劳部 |
|
Cite this article:
Yongde LI; shou xin LI. The influence of hydrogen on ultra-high cycle fatigue properties of high strength spring steel 50CrV4. Acta Metall Sin, 2008, 44(1): 64-68 .
|
|
|
Abstract The influence of hydrogen on ultra-high cycle fatigue (UHCF) properties of high strength spring steel was discussed in this study. Three groups of specimens with different hydrogen content (CH) were obtained from three different heat treatment procedures: quenched and tempered (specimen QT), annealed at 380℃ in a vacuum after QT (specimen VA) and treated by High-pressure Thermal Hydrogen Charging (HPTHC) after QT (specimen HPTHC). It was observed by SEM that the crack initiation site was internal inclusion clusters for a high cycle fatigued specimen . The fatigue strength (σw) decreased according to σ0-аexp(CH)law with the increase of CH. Basquin exponent--b in Basquin Eq. decreased gradually with the increase of CH.
|
|
Received: 23 July 2007
|
|
|
[1]Chapetti M D,Tagawa T,Miyata T.Mater Sci Eng,2003; A356:227 [2]Bathias C.Fatigue Fract Eng Mater Struct,1999;22:559 [3]Wang Q Y,Berard J Y,Dubarre A,Baudry G.,Rathery S,Bathias C.Fatigue Fract Eng Mater Struct,1999;22: 667 [4]Murakami Y,Nomoto T,Ueda T.Fatigue Fract Eng Mater Struct,2000;23:893 [5]Shiozawa K,Morii Y,Nishino S,Lu L.Int J Fatigue,2006; 28:1521 [6]Murakami Y,Matsunaga H.Int J Fatigue,2006;28:1509 [7]Li X Y,Li Y Y.The Hydrogen Damage of Austenite Al- loys.Beijing:Science Press,2003:83 (李秀艳,李依依.奥氏体合金的氢损伤.北京:科学出版社,2003:83) [8]Chu W Y,Qiao L J,Chen Q Z.Fracture and Environ- mental Fracture.Beijing:Sciences Press,2000:101 (褚武扬,乔立杰,陈奇志.断裂与环境断裂.北京:科学出版社,2000:101) [9]Li X Y,Li Y Y.The Hydrogen Damage of Austenite Al- loys.Beijing:Science Press,2003:1 (李秀艳,李依依.奥氏体合金的氢损伤.北京:科学出版社,2003:1) [10]Wang M Q,Akiyama E,Tsuzaki K.Scr Mater,2005;52: 403 [11]Zhang J M,Li S X,Yang Z G.,Li G.Y,Hui W J,Weng Y Q.Int J Fatigue,2007;29:765 [12]Yang Z G,Zhang J M,Li S X,Li G Y,Hui W J,Weng Y Q.Mater Sci Eng,2006;A427:167 [13]Suresh S,Translate by Wang Z G,et al.Fatigue of Mate- rials.2nd Ed.,Beijing:National Defence Industry Press, 1999:157 (Suresh S著;王中光,等译.材料的疲劳.第2版,北京:国防工业出版社,1999:157) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|