| PITT investigation of apparent diffusion of lithium-ion through PLD-deposited HT-LiCoO2 films |
| ZHANG Yao;Chi-Yuen CHUNG; |
| 华南理工大学机械学院 |
|
Cite this article:
ZHANG Yao; Chi-Yuen CHUNG. PITT investigation of apparent diffusion of lithium-ion through PLD-deposited HT-LiCoO2 films. Acta Metall Sin, 2007, 43(8): 818-822 .
|
|
|
Abstract In this work, LiCoO2 films were prepared with the pulsed laser deposition (PLD) method. Their structure was characterized by X-ray diffraction, Raman spectra and Scanning electron microscopy and their electrochemical properties were evaluated with cyclic voltammetry (CV). Results showed that LiCoO2 films prepared with PLD at 600℃ had a well-crystallized columnar HT-LiCoO2 structure with the average grain size less than 100nm and with a strong [001] preferred orientation, while these films contain trace amount of Co3O4. CV tests indicated that PLD-deposited HT-LiCoO2 films had good electrochemical reversibility but only a pair of redox peaks near 3.9V(vs Li) were observed in the cyclic voltammograms. Thereafter, emphasis was laid on the study of apparent diffusion of lithium-ion through LiCoO2 films using the potentiostatic intermittent titration technique (PITT). PITT measurements revealed that the lithium-ion diffusion coefficient of PLD-deposited HT-LiCoO2 films reached 10-8~10-9cm2s-1, 1-2 orders of magnitude faster than those prepared by other methods including R.F. magnetron sputtering and, in the voltage range between 3.85~3.95V(vs Li), the lithium-ion diffusion coefficient of PLD-deposited HT-LiCoO2 films was 1-2 orders of magnitude lower than other voltage ranges. The former should be ascribed to the grain refinement of PLD-deposited HT-LiCoO2 films and existence of many voids, while the later may due to the hindrance arising from phase boundary movement.
|
|
Received: 04 December 2006
|
|
|
[1]Reimers J N,Dahn J R.J Electrochem Soc,1992;39:2091 [2]Bueno P R,Leite E R.J Phys Chem,2003;107B:8868 [3]Wang B,Bates J B,Hart F X,Sales B C,Zuhr R A, Robertson J D.J Electrochem Soc,1996;143:3203 [4]Polo da Fonseca N,Davalos J,Kleinke M,Fantini M C A, Gorenstein A.J Power Sources,1999;81-82:575 [5]Kim W S.J Power Sources,2004;134:103 [6]Liao C L,Fung K Z.J Power Sources,2004;128:263 [7]Iriyama Y,Inaba M,Abe T,Ogumi Z.J Power Sources, 2001;94:175 [8]Julien C,Camacho-Lopez M A,Alarcon L E,Poniatowski E H.Mater Chem Phys,2001;68:210 [9]Perkins J D,Bahn C S,McGraw J M,Parilla P A,Ginley D S.J Electrochem Soc,2001;148A:1302 [10]Bouwman P J,Boukamp B A,Bouwmeester H J M,Not- ten P H L.J Electrochem Soc,2002;149A:699 [11]Tang S,Lu L,Lai M O.Philos Mag,2005;85:2831 [12]Xia H,Lu L,Ceder G.J Alloys Compd,2006;417:304 [13]Cho S I,Yoon S G.J Electrochem Soc,2002;149A:1584 [14]Kushida K,Kuriyama K.J Cryst Growth,2002;237-239: 612 [15]Kim K W,Woo S I,Choi K H,Han K S,Park Y J.Solid State Ionics,2003;159:25 [16]Chen C H,Kelder E M,Jak M J G,Schoonman J.Solid State Ionics,1996;86-88:1301 [17]Shin H C,Pyun S I.Electrochim Acta,2001;46:2477 [18]Xia H,Lu L,Ceder G.J Power Sources,2006;159:1422 [19]Montella C.Electrochim Acta,2006;51:3102 [20]Wen C J,Boukamp B A,Huggins R A.J Electrochem Soc, 1979;126:2258 [21]Aurbach D,Levi M D,Levi E,Teller H,Markovsky B, Salitra G,Heider U,Heider L.J Electrochem Soc,1998; 145:3024 [22]Peng W J,Li X H,Wang Y Y,Wang Z X,Guo H J.J Cent South Univ(Sci Technol),2004;35:568 (彭文杰,李新海,王云燕,王志兴,郭华军.中南大学学报(自然科学版),2004;35:568) |
| No Suggested Reading articles found! |
|
|