Abstract  High pressure gas atomization experiments were done with Al-Pb immiscible alloy. Powders with a Pb-rich shell on their surfaces were obtained. A model describing the microstructure evolution in Al-Pb atomized droplet was developed. The solidification process was calculated. The results indicate that the formation of the shell-type structure is due to the heterogeneous nucleation of the Pb-rich phase on the atomized drop surface.
Key words:       
Received:  30 October 2006     
ZTFLH:  TG113.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I6/659

[1]Jia J,Zhao J Z,Guo J J,Liu Y.Immiscible Alloys and Their Manufacturing Technique.Harbin:Press of Harbin Institute of Technology,2002:1 (贾均,赵九洲,郭景杰,刘元.难混熔合金及其制备技术.哈尔滨,哈尔滨工业大学出版社,2002:1)
[2]Wang C P,Liu X J,Ohnuma I,Kainuma R,Ishida K. Science,2002;297:990
[3]Bradley E,Banerji K.IEEE Trans Compon Packag Manuf Technol,1996;19B:320
[4]Wilde G,Perepezko J H.Acta Mater,1999;47:3009
[5]Zhao J Z.Scr Mater,2006;54:247
[6]Liu D M,Zhao J Z,Ye H Q.Acta Metall Sin,2003;39: 375 (刘东明,赵九洲,叶恒强.金属学报,2003;39:375)
[7]Christian J.The Theory of Phase Transformation in Met- als and Alloys.2nd,Elmsford,NY:Pergamon Press, Vol.1,1975:422
[8]Wynblatt P,Saul A,Chatain D.Acta Mater,1998;46: 2337
[9]Zhao J Z,Ratke L,Feuerbacher B.Modell Simul Mater Sci Eng,1998;6:123
[10]Tao W Q.Numerical Heat Transfer.Xi'an:Xi'an Jiao- tong University Press,2001:1 (陶文铨.数值传热学.西安交通大学出版社,2001:1)
[11]Yu S K,Sommer F,Predel B.Z Metallkd,1996;87:574
[12]Zhao J Z,Ratke L.Sct Mater,2004;50:543
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!