Please wait a minute...
Acta Metall Sin  2007, Vol. 43 Issue (6): 612-618     DOI:
Research Articles Current Issue | Archive | Adv Search |
Cite this article: 

. . Acta Metall Sin, 2007, 43(6): 612-618 .

Download:  PDF(871KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  To understand the alloying effects of a heavy rare earth metal, ytterbium, in magnesium, two series of Mg-Yb and Mg-Yb-0.5Zr magnesium alloys were prepared using flux protection with Yb additions of 0.5, 1, 2, 3, 4 and 8 % (mass fraction), respectively. Microstructure analyses and mechanical properties tests of the alloys were performed by use of optical microscope, X-ray diffraction, differential scanning calorimeter, Scanning electric microscope and electro-probe, et al. It is found that adding ytterbium in pure Mg can refine grain sizes remarkably but not change the primary columnar morphology below 4% Yb contents. All Mg-Yb binary alloys obtained fine equiaxed grains with the addition of 0.5% (mass fraction) zirconium. The tensile strengths and hardness of the alloys increase with the increase of Yb contents. In the case of high Yb content, 8%, the strength and elongation drops sharply due to the formation of continuous network Mg2Yb intermetallics and eutectic structures on grain boundaries. The results show that ytterbium has refining and alloying effects on magnesium and zirconium was an effective grain refiner in Mg-Yb binary alloys.
Key words:       
Received:  30 October 2006     
ZTFLH:  TG113.12, TG146.2  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I6/612

[1]Mordike B L,Ebert T.Mater Sci Eng,2001;A302:37
[2]Zheng W C,Li S S,Tang B,Zeng D B.Acta Metall Sin, 2006;42:835 (郑伟超,李双寿,汤彬,曾大本.金属学报,2006;42:835)
[3]Xia C Q,Wang Y N,Wu A R,Gu Y.J Central South Univ Technol,2005;12:515
[4]Rokhlin L L,Dobatkina T V,Tarytina I E.J Alloy Compd, 2004;367:17
[5]Li Z C,Zhang H,Liu L.Mater Lett,2004;58:3021
[6]Ma C J,Liu M P,Wu G H.Mater Sci Eng,2003;A349: 207
[7]Ye C W,Liu Z Y,Zhang K.Foundry,2005;54:356 (叶呈武,刘志义,张坤.铸造,2005;54:356)
[8]Rokhlin L L,Nikitina N I.J Alloy Compd,1998;279:166
[9]Nie J F,Gao X,Zhu S M.Scr Mater,2005;53:1049
[10]Massalski T B,Murray J L,Bennett L H.Binary Alloy Phase Diagrams.Materials Park,Ohio:ASM,1988:1563
[11]Li D H,Dong J,Zeng X Q.Mater Rev,2005;19(8):51 (李德辉,董杰,曾小勤.材料导报,2005;19(8):51)
[12]Ferro R,Saccone A,Borzone G.J Chin Rare Earth Soc, 1997;15:262 (Ferro R,Saccone A,Borzone G.中国稀土学报,1997;15: 262)
[13]Lu S Q,Huang B Y,He Y H.Mater Rev,2003;17(1):11 (鲁世强,黄伯云,贺跃辉.材料导报,2003;17(1):11)
[14]Yu K,Li W X,Zhang S J.Rare Met Mater Eng,2005;7: 1013 (余琨,黎文献,张世军.稀有金属材料与工程,2005;7: 1013)
[15]Luo Z P,Zhang S Q.Acta Metall Sin,1993;29:176 (罗治平,张少卿.金属学报,1993;29:176)
[16]Ma Q,Das A.Scr Mater,2006;54:881h
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!