INVESTIGATION OF RAPID DIRECTIONAL SOLIDIFICATION OF AL-BASED IMMISCIBLE ALLOYS Ⅲ. EFFECT OF SOLID/LIQUID INTERFACE
Jie He;;;;;
金属研究所
Cite this article: 

Jie He. INVESTIGATION OF RAPID DIRECTIONAL SOLIDIFICATION OF AL-BASED IMMISCIBLE ALLOYS Ⅲ. EFFECT OF SOLID/LIQUID INTERFACE. Acta Metall Sin, 2007, 43(6): 561-566 .

Download:  PDF(455KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The forces acting on the sphere in front of the S/L interface during the solidification of immiscible alloys have been analyzed. The dynamic criterion for the interaction mode between the sphere and solidification interface has been proposed. Combining theory with experiment, the effect of the interaction between the S/L interface and the sphere on the microstructure development in the Al-Bi based immiscible alloy has been discussed in detail. The results have indicated that the small Bi-rich spheres were repelled and accumulated in front of the solidification interface due to the combined action of the interfacial repulsion and Marangoni migration. If the interface morphology is dendritic or cellular, the Bi-rich sphere with critical size is partially entrapped by the interface and forms tadpole-type particle. While, the smaller Bi-rich spheres will be entrapped in the interdendrite and the Bi-rich particles distribute at the grain boundaries and the triple junctions after solidification.
Key words:       
Received:  09 November 2006     
ZTFLH:  TG146  
  TG224  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I6/561

[1]K(?)rber C,Rau G,Cosman M D,Cravalho E G.J Cryst Growth,1985;72:649
[2]Stefanescu D M,Dhindaw B K,Ahuja S.Metall Trans, 1988;19A:2847
[3]Juretzko F R,Dhindaw B K,Stefanescu D M,Sen S,Cur- reri P A.Metall Trans,1998;29A:1691
[4]Kennedy A R,Clyne T W.Cast Met,1991;4:160
[5]He J,Zhao J Z,Ratke L.Acta Mater,2006;54:1749
[6]He J,Zhao J Z,Wang X F,Gao L L.Metall Mater Trans, 2005;36A:2449
[7]He J,Zhao J Z.Acta Metall Sin,2005;41:407 (何杰,赵九洲.金属学报,2005;41:407)
[8]Zhong Y B,Ren Z M,Sun Q X,Jiang Z W,Deng K,Xu K D.Acta Metall Sin,2003;39:1269 (钟云波,任忠鸣,孙秋霞,江志文,邓康,徐匡迪.金属学报,2003;39:1269)
[9]Asthana R,Tewari S N.J Mater Sci,1993;28:5414
[10]Monti R, Savino R,Alterio G.Acta Astronaut,2002;51: 789
[11]Kaptay G.Mater Sci Forum,2006;508:269
[12]Uhlmann D R,Chalmers B,Jackson K A.J Appl Phys, 1964;35:2986
[13]Kim J M,Rohatgi P K.Mater Sci Eng,1998;A244:168
[14]Beshkov V N,Radoev B P,Ivanov I B.Int J Multiphase Flow,1978;4:563
[15]Dutta B,Surappa M K.Metall Mater Trans,1998;29A: 1329
[16]Coupard D,Girot F,Quenisset J M.J Mater Sci,1996; 31:5305
[17]Zubko A M,Lobanov V G,Nikonova V V.Soviet Phys Crystallogr,1973;18:239
[18]Shangguan D,Ahuja S,Stefanescu D M.Metall Trans, 1992;A23:669
[19]He J.PhD Dissertation,Institute of Metal Research,Chi- nese Academy of Sciences,Shenyang,2006 (何杰.中国科学院金属研究所博士学位论文,沈阳,2006)
[20]Geiger G H,Poirier D R.Transport Phenomena in Met- allurgy.London:Addison-Wesley,1973
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!