Effects of Al2O3 and Cr Interlayers on the Optical Property and Adhesion of Ag Film |
|
Cite this article:
. Effects of Al2O3 and Cr Interlayers on the Optical Property and Adhesion of Ag Film. Acta Metall Sin, 2007, 43(3): 307-310 .
[1]Wu G F,Song x P,Yang C H,Jiang B,Sun Z Q.Funct Mater,2003;34:682 (吴桂芳,宋学萍.杨成浩,江兵,孙兆奇.功能材料,2003; 34:682) [2]Wei Q Y,Yu S G.Precious Met,2001;22(2):5 (韦群燕,俞守耕.贵金属,2001;22(2):5) [3]Xie Z W,Meng J L,Wang G Q.Vac Sci Technol,2001; ??21:203 (谢致薇.蒙继龙,王国庆.真空科学与技术,2001;21:203) [4]Aoshima Y,Miyazaki M,Sato K,Akao Y,Takaki S, Adachi K.Jpn J Appl Phys,2000;39:4884 [5]Alford T L,Adams D,Laursen T,Manfred U B.Appl Phys Lett,1996;68:3251 [6]Xu X K,Tang Z S,Fan Z X,Shao J D.Opt Eng,2004; 43:971 [7]Tian M B,Liu D L.Handbook of Science and Technology of Thin Film.Beijing:China Machine Press,1991 (田民波,刘德令.薄膜科学与技术手册.北京:机械工业出版社,1991) |