MICROSCOPIC PHASE-FIELD SIMULATION COUPLED WITH ELASTIC STRAIN ENERGY FOR γ′(Ni3Al) PRICIPITATION IN Ni-Al ALLOY
LU Yanli; CHEN Zheng;LI Yongsheng; WANG Yongxin
School of Materials Science and Engineering; Northwestern Polytechnical University; Xi'an 710072
Cite this article: 

LU Yanli; CHEN Zheng; LI Yongsheng; WANG Yongxin. MICROSCOPIC PHASE-FIELD SIMULATION COUPLED WITH ELASTIC STRAIN ENERGY FOR γ′(Ni3Al) PRICIPITATION IN Ni-Al ALLOY. Acta Metall Sin, 2007, 43(3): 291-296 .

Download:  PDF(781KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the microscopic phase-field dynamic model and the microelasticity theory, the morphology evolution of γ′ phase(Ni3Al)and early precipitation mechanism in Ni-Al alloy were studied. Simulation results show that γ′ phase changes from initial circular or irregular shape into the quadrate shape and their orientations become more obvious during precipitation process, in the later stage, the γ′ precipitates present quadrate shape with round corner and regularly align along the [10] and [01] directions. Under the effect of elastic strain energy, the coarsening process follows the rule of preferential election, the particles lying in the elastic soft directions grow and coarsen further; the particles lying out of the elastic soft direction shrink and dissolve, highly preferential selected microstructure is formed in the later precipitation process. The early precipitation mechanism is the non-classical nucleation and growth, the evolution of γ′ phase is in the order: supersaturated solid solution→nonstoicheometric ordered phase→stoicheometric γ′ phase→growth.
Key words:  Ni-Al alloy      γ′ phase      elastic strain energy      precipitation process      
Received:  14 July 2006     
ZTFLH:  TG111.5  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I3/291

[1]Wendt H,Hassen P.Acta Metall,1993;31:1649
[2]Banerjee D,Banerjee R,Wang Y.Scr Mater,1999;41: 1023
[3]Vaithyanathan V,Chen L Q.Acta Mater,2002;50:4061
[4]Sob J R,Lee H M.Acta Mater,1997;45:4743
[5]Ardell A J,Maheshwari A.Acta Metall Mater,1995;43: 1825
[6]Miyazaki T.Mater Trans,2002;43:1266
[7]Vaithyanathan V,Chen L Q.Acta Mater,2002;50:4061
[8]Wen Y H,Chen L Q,Hazzledine P M,Wang Y.Acta Mater,2001;49:2341
[9]Khachatuyran A G.Theory of Structural Transformations in Solids.New Tork:Wiley,1983:23
[10]Jiang Z H,Wang Y X,Chen Z.Acta Metall Sin,2004;40: 616 (江志华,王永欣,陈铮.金属学报,2004;40:616)
[11]Miyazaki T,Koyama T,Kozakai T.Mater Sci Eng,2001; A312:8
[12]Shen C,Simmons J P,Wu K,Wang Y.Materials De- sign Approaches and Experiences.Warrendale,PA:TMS, 2001:57
[13]Poduri R,Chen L Q.Acta Mater,1997;45:245
[14]Miyazaki T,Koyama T,Kozakai T.Mater Sci Eng,2001; A312:38
[15]Li X L,Chen Z,Liu X G,Liu B.Acta Metall Sin,2002; 38:458 (李晓玲,陈铮,刘晓光,刘兵.金属学报,2002;38:458)
[16]Pareige C,Blavette D.Scr Mater,2001;44:243
[17]Prikhodko S V,Carnes J D,Isaak D G,Ardell A J.Scr Mater,1998;38:67
[18]Qiu Y Y.Acta Mater,1996;44:4969
[19]Chen L Q,Khachaturyan A G.Scr Metall,1991;25:67
[1] HAN Guomin, HAN Zhiqiang, Alan A. Luo, Anil K. Sachdev, LIU Baicheng. PHASE FIELD SIMULATION ON MORPHOLOGY OF CONTINUOUS PRECIPITATE Mg17Al12IN Mg-Al ALLOY[J]. 金属学报, 2013, 49(3): 277-283.
[2] ZHOU Guangzhao, WANG Yongxin, CHEN Zheng. PHASE-FIELD METHOD SIMULATION OF THE EFFECT OF ELASTIC STRAIN ENERGY ON COARSENING DYNAMICS DURING THE α2→ O PHASE TRANSFORMATION IN Ti-Al-Nb ALLOYS[J]. 金属学报, 2012, 48(4): 485-491.
No Suggested Reading articles found!