Abstract The mathematical model of cathodic protection potential distribution on the exterior of tank bottom is established and cathodic polarization performance is described according to the mixed polarization theory. The cathodic protection potential distribution on the exterior of tank bottom under protection of different kinds of anode placement manners is calculated by FLUENT software and the effects of soil resistivity and tank diameter on potential distribution are studied and compared also. The results can provide theoretical guidance for determining cathodic protection effects and choosing anode placement manners.
|
Received: 08 June 2006
|
|
[1]Degiorgi V G,Wimmer S A.Eng Anal Bound Elem,2005; 29:15 [2]Degiorgi V G,Thomas E D,Lucas K E.Eng Anal Bound Elem,1998;22:41 [3]Zamani N G.Appl Math Comp,1988;26:119 [4]Bialecki R A,Ostrowski Z,Kassab A J,Yin Q,Sciubba E.Eng Anal Bound Elem,2002;26:597 [5]Santiago J A F,Tells J C F.Adv Eng Software,1999;30: 663 [6]Hassanein A M,Glass G K,Buenfeld N R.Cement Con- crete Compos,2002;24:159 [7]Degiorgi V G.Eng Anal Bound Elem,2002;26:435 [8]Kranc S C,Alberto A S.Corros Sci,2001;43:1355 [9]Qiu F,Xu N X.J Chin Soc Corros Prot,1997;17:106 (邱枫,徐乃欣.中国腐蚀与防护学报,1997;17:106) [10]Qiu F,Xu N X.J Chin Soc Corros Prot,1997;17:12 (邱枫,徐乃欣.中国腐蚀与防护学报,1997;17:12) [11]Zhang M D,Du Y L,Yin Z A,Liu M,Ge W L.J Chin Soc Corros Protect.1994;14:77 (张鸣镝,杜元龙,殷正安,刘曼,葛文林.中国腐蚀与防护学报,1994;14:77) [12]Qian H J,Liu X G,Zhang S X,Tao Y S,Xiao S M.Chem Eng Mach,1997;24:281 (钱海军,刘小光,张树霞,陶永顺,肖世猛.化工机械,1997; 24:281) [13]Liu M,Yin Z A,Zhan G S,J Dalian Univ Technol,1998; 38:599 (刘曼,殷正安,战广深.大连理工大学学报,1998;38:599) [14]Liang X W,Wu Z Y,Liu Y H,Di Z.J Tianjin Inst Textile Sci Technol,1999;18(1):37 (梁旭魏,吴中元,刘燕华,狄峥.天津纺织工学院学报,1999; 18(1):37) [15]Liang X W,Wu Z Y,Meng X J,Zhuang X G.J Tianjin Inst Textile Sci Technol,1998;17(5):90 (梁旭魏,吴中元,孟宪级,庄新国.天津纺织工学院学报,1998; 17(5):90) [16]Qiu F,Xu N X.J Chin Soc Corros Prot,1996;16:29 (邱枫,徐乃欣.中国腐蚀与防护学报,1996;16:29) [17]Ma W P,Zhang G Z,Liang C H,Zhang D P.Oil Gas Storage Transpo,2004;23(9):31 (马伟平,张国忠,梁昌华,张大鹏.油气储运.2004;23(9): 31) [18]Ma W P,Zhang G Z,Liang C H,Zhang D P,Li B D,An Z S,Nat Gas Oil,2004;22(4):18 (马伟平,张国忠,梁昌华.张大鹏.李柏丹,安振山.天然气与石油,2004;22(4):18) [19]Douglas P R,Mark E O.Corros Sci,2005;47:849 [20]Cao C N.Corrosion Electrochemistry Theory.Beijing: Chemical Industry Press.2004:60 (曹楚南.腐蚀电化学原理.北京:化学工业出版社,2004:60) [21]Sun J B.Oil Gas Storage Transpo,2001;20(1):23 (孙建斌.油气储运,2001;20(1):23) [22]Sun J B.Oil Depot Gas Station,2001;10(1):31 (孙建斌.石油库与加油站,2001;10(1):31) |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|