| The formation mechanism of band-like microstructures in directionally solidified Cu-1.0%Cr hypoeutectic alloy |
| LI Xiao-Li;;;; |
| 西北工业大学凝固技术国家重点实验室 |
|
Cite this article:
LI Xiao-Li. The formation mechanism of band-like microstructures in directionally solidified Cu-1.0%Cr hypoeutectic alloy. Acta Metall Sin, 2007, 43(12): 1256-1260 .
|
|
|
Abstract Band-like microstructures were observed in directionally solidified Cu-1.0%Cr hypoeutectic alloy at the growth rate ranging from 2m/s to 10m/s and the temperature gradient of 200K/cm in liquid. There are three kinds of band-like microstructures, which are the planar interface plus coupled eutectic, the planar interface plus cellular structure with the growth of coupled eutectic, and cellular interface structure plus coupled eutectic, respectively. The formation mechanism of band-like microstructures has been illustrated by discussing the solute distribution ahead of solid-liquid interface in which the growth rate and alloy composition are changed at the non-steady state in directional solidification. In addition, the density difference between Cu phase and Cr phase is also an available factor to cause the formation of band-like microstructures in directionally solidified Cu-1.0%Cr hypoeutectic alloy.
|
|
Received: 07 February 2007
|
|
|
[1]Burden M H,Hunt J D.J Cryst Growth,1974;22:109 [2]Karma A,Sarkissian A.Metall Mater Trans,1996;27A: 635 [3]Hunziker O,Vandyoussefi M,Kurz W.Acta Mater,1998; 46:6325 [4]Kerr H W,Kurz W.Int Mater Rev,1996;41:129 [5]Han S H,Trivedi R.Metall Mater Trans,2000;31A:1819 [6]Karma A,Rappel W J,Fuh B C,Trivedi R.Metall Mater Trans,1998;29A:1457 [7]Tokieda K,Yasuda H,Ohnaka I.Mater Sci Eng,1999; A262:238 [8]Li S M,Liu L,Li X L,Fu H Z.Acta Metall Sin,2004;40: 20 (李双明,刘林,李晓历,傅恒志.金属学报,2004;40:20) [9]Li X Z,Guo J J,Su Y Q,Wu S P,Fu H Z.Acta Metall Sin,2005;41:593 (李新中,郭景杰,苏彦庆,吴士平,傅恒志.金属学报,2005;41:593) [10]Guo J J,Li X Z,Su Y Q,Wu S P,Fu H Z.Acta Metall Sin,2005;41:599 (郭景杰,李新中,苏彦庆,吴士平.傅恒志.金属学报,2005;41:599) [11]Liu P,Jia S G,Zhao D M,Ken F Z,Tian B H,Kang B X.Mater Rev,2004;18(6):32 (刘平,贾淑果,赵冬梅,任凤章,田保红,康布熙.材料导报,2004;18(6):32) [12]Bi X Q,Hu R,Li J S,Zhu Q,Fu H Z.Mater Sci Technol, 2005;13:153 (毕晓勤,胡锐,李金山,朱琦,傅恒志.材料科学与工艺,2005;13:153) [13]Hu R,Bi X Q,Li J S,Fu H Z.Sci Technol Adv Mater, 2005;6:950 [14]Carroll H E,Whitehouse A F.Set Mater,2000;42:1133 [15]Yu J Q,Yi W Z,Chen B D,Chen H J.Phase Diagram of Binary Alloy.Shanghai:Shanghai Science and Technol- ogy Press,1987:318 (虞觉奇,易文治,陈邦迪,陈宏鉴.二元合金相图集.上海:上海科学技术出版社,1987:318) [16]Tiller W A,Jackson K A,Rutter J W,Chalmers B.Acta Metall,1953;1:428 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|