Cite this article: 

. . Acta Metall Sin, 2007, 43(11): 1181-1185 .

Download:  PDF(989KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Abstract: Wettability of PdNi-Cr-V alloy on SiC was studied with the sessile drop method. The newly-developed PdNi-(10-25)Cr-(5-25)V-Si-B brazing filler could be used for joining SiC. The room-temperature three-point bend strength of the SiC/SiC joints brazed with the rapidly-solidified brazing foils at 1190℃ for 10 min is 84.6 MPa. In the interfacial layer near to SiC, elements Pd and Ni preferentially diffused to SiC and resulted in the reaction products of Pd-Si phase, Ni-Si phase and graphite. In the reaction zone further away from the SiC, mainly elements Cr and V in the brazing filler participated in the interface reaction, and formed Cr(V)-C, Cr(V)-Si, Cr(V)5Si3C. In the central part of the joint, the matrix was composed of Pd-Si, Ni-Si and V-Si phases, on which some blocky carbides V2C, Cr23C6 distributed scatteringly.
Key words:       
Received:  16 January 2007     
ZTFLH:  TG146  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I11/1181

[1]Okamura H.Weld Int,1993;7:263
[2]Nishino T,Urai S,Okamoto I,Naka M.Weld Int,1992; 6:600
[3]Lee Y K,Lee J Y.J Mater Sci,1996;31:4133
[4]Xiao P,Derby B.Acta Mater,1998;46:3491
[5]Naka M,Taniguchi H,Okamoto I.Trans JWRI,1990; 19(11):25
[6]Fukai T,Liu Y L,Naka M.Trans Chin Weld Soc,1998; 19(2):93 (深井卓,刘玉莉,奈贺正明.焊接学报,1998;19(2):93)
[7]Liu Y L,Feng J C,Naka M.J Harbin Inst Technol,1998; 30(6):61 (刘玉莉,冯吉才,奈贺正明.哈尔滨工业大学学报,1998;30(6):61)
[8]Chou T C.Scr Metall Mater,1993;29:255
[9]McDermid J R,Drew R A L.J Am Ceram Soc,1991;74: 2055
[10]Xiong H P,Chen B,Kang Y S,Mao W,Kawasaki A, Okamura H,Watanabe R.Scr Mater,2007;56:173
[11]Xiong H P,Mao W,Cheng Y Y,Li X H.Acta Metall Sin, 2001;37:991 (熊华平,毛唯,程耀永,李晓红.金属学报,2001;37:991)
[12]Park J S,Landry K,Perepezko J H.Mater Sci Eng,1999; A259:279
[13]Gulpen J H,Kodentsov A A,Loo F J J.Z Metallkd,1995; 86:530
[14]Bhanumurthy K,Schmid-Fetzer R.Composites,2001; 32A:569
[15]Fukai T,Naka M,Schuster J C,Okamoto I.Trans JWRI, 1997;26(1):93
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!