Abstract Researches on the antibacterial properties and relevant mechanism of copper-contained ferritic and austenitic antibacterial stainless steels have been made in this paper. Experimental results displayed that copper-contained antibacterial stainless steels have the broad-spectrum antibacterial functions, and the antibacterial rate against most of the Gram-negative bacteria and Gram-positive bacteria in the present work reached above 99.0%. Through research on the different action time of E.coli in contact with ferritic antibacterial stainless steel, it was proved that the antibacterial rate of a stainless steel was related to the action time, and the antibacterial rate reached 99.9% only when the steel contacted with the bacteria for about 150min. The observation on AFM indicated that the antibacterial mechanism of the antibacterial stainless steels should be attributed to leaking of the contents and shriveling of the cells in the bacteria . The electrochemical experiments showed that after contacted with E.coli, the dissolution of Cu ions on the surface of antibacterial stainless steels became faster, resulting in a decrease of the pitting potential of the steel.
|
|
Received: 01 February 2007
|
|
|
[1]Cao F Q,Kong L,Yang S L.J China Today Med,2003; 3(13):91 (曹芳芹,孙琳,杨胜利.中华今日医学杂志,2003;3(13):91) [2]Lu D Y.Medical Microbiology.5ed,Beijing:People San- itation Publishing,2001:28 (陆德源.医学微生物学.第5版,北京:人民卫生出版社,2001:28) [3]Ellis G P,Luscombc D K.Prog Med Chem,1994;81:351 [4]Wu X H,Yang L F,Wang Y D,Zhao J C.1st Inter- national Exhibition of China Antibacterial Products,2nd Developing Conference of China Antibacterial Materials Industries,Beijing,2002:235 (吴兴惠,杨留方,王毓德,赵景畅.见:中国首届抗菌制品(材料)国际展览会,第二届中国抗菌材料产业发展大会,北京,2002:235) [5]Shi K.High Seminar of Chinese Public Sanitation Con- struction,Beijing:National Hcalth Industry Business Management Association,2004:148 (时勘.见中国公共卫生建设高层研讨会,北京:全国卫生产业企业管理协会,2004:148) [6]Wan Y Z,Wamg Y L,Cheng G X,Yao K D,Tao H M, Xin J Y,Wen T Y.Mater Sci Eng,1998;16(4):2 (万怡灶,王玉林,成国祥,姚康德,陶海明,辛景义,温廷益.材料科学与工程,1998;16(4):2) [7]Zhong F L,Cao H B,Li X G.Mater J,2000;14(8):43 (钟方丽,曹宏斌,李鑫钢.材料导报,2000;14(8):43) [8]Wright J B,Lam K,Burrell R E.Am J Infect Control, 1998;26:572 [9]Chen S H.PhD Dissertation,Institute of Metal Research, Chinese Academy of Sciences,Shenyang,2004 (陈四红.中国科学院金属研究所博士学位论文,沈阳,2004) [10]Chen S H,LüM Q,Zhang J D,Dong J S,Yang K.Acta Metall Sin,2004;40:314 (陈四红,吕曼祺,张敬党,董加胜,杨柯.金属学报,2004;40:314) [11]LüM Q,Chen S H,Dong J S,Yang K.Chin J Mater Res, 2005;19:581 (吕曼祺,陈四红,董加胜,杨柯.材料研究学报,2005;19:581) [12]Yang K,Dong J S,Chen S H,LüM Q.Chin J Mater Res, 2006;20:523 (杨柯,董加胜,陈四红,吕曼祺.材料研究学报,2006;20:523) [13]Chen S H,LüM Q,Yang K,Dong J S,Zhang J D,Wu P S.Chin Pat 02144683.0,2002 (陈四红,吕曼祺,杨柯,董加胜,张敬党,吴平森.一种奥氏体抗菌不锈钢,中国发明专利,02144683.0,2002) [14]Chen S H,LüM Q,Yang K,Zhang J D,Wu P S.Chin Pat 02144568.0.2002 (陈四红,吕曼祺,杨柯,张敬党,吴平森.中国发明专利,02144568.0,2002) [15]Ji J H,Shi W M.Antibacterial Mater.Beijing:Mate- rial Science and Engineering Center of Chemical Industrial Press,2003:1 (季军晖,史维明.抗菌材料.北京:化学工业出版社材料科学与工程出版中心,2003:1) [16]State Bureau of Technology Supervision.GB 8537—1995. Beijing:Standards Press of China,1995 (国家技术监督局.GB 8537—1995.北京:中国标准出版社,1995) [17]PRC Bureau of National Quality Supervision and Inspec- tion Quarantine.GB 17324—2003.Beijing:Standards Press of China,2003 (中华人民共和国国家质量监督检验检疫总局.GB 17324- 2003.北京:中国标准出版社,2003) [18]Zhang P Y,Liu W M,Xue Q J.Elect Microtrans,2000; 19:593 (张平余,刘维民,薛群基.电子显徼学报,2000;19:593 [19]Yokota T,Tochibara M,Ohta M.Kawasaki Steel Technol Rep,2002;46:37 [20]Dan Z G,Ni H W,Xu B F,Xiong J,Xiong P Y.Thin Solid Film,2005;492:95 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|