Abstract  Using the first-principles self-consistent discrete variational method (DVM) based on density functional theory, we investigated the effect of impurity S on the electronic structure of the kink on the [100](010) edge dislocations(ED) in bcc iron. We calculate the segregation energy, the interatomic energy, the local density of states and the charge density. The results show that S obtains electrons from its neighboring Fe atoms when a S atom is introduced into interstitial sites in the kink. It is found that there are the strong hybridizations between impurity S-d with Fe-3d4s4p states. The interaction between impurity S atom and neighboring Fe atoms are strengthen, while the interaction between the host Fe atoms are decreased, which is beneficial to the migration of kink. The bonding between the impurity S and the host Fe atoms are mainly ascribed to contribution of p and d states, which leads to the bonding between them has strong orientation, and the strength and toughness of materials both are decreased.
Key words:       
Received:  12 December 2006     
ZTFLH:  TG111.2  
  TG142.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I10/1015

[1]Yan J A,Wang C Y,Duan W H,Wang S Y.Phys Rev, 2004;59B:214110
[2]Niu Y,Zhao D L,Wang C Y.Acta Metall Sin,2001;37: 239 (牛原,赵栋梁,王崇愚.金属学报,2001;37:239)
[3]Feng Y Q,Wang C Y.J Alloy Compd,2000;312:219
[4]Alexander H.In:Nabarro F R N ed.,Dislocation in Solids. Amsterdam:North-Holland,1986:115
[5]Gornostyrev Y N,Katsnelson M I,Stroev A Y,Trefilov A V.Phys Rev,2005;71B:094105
[6]Wen M,Fukuyama S,Yokogawa K.Acta Mater,2003;51: 1767
[7]Chen L Q,Qiu Z C,Wang C Y,Yu T.J Alloy Compd, 2007;428:49.
[8]Chen L Q,Qiu Z C.Defect Diffus Forum,2007;261:37
[9]Ellis D E,Benesh G A,Byrom E.Phys Rev,1977;16B: 3308
[10]Guenzburger D,Ellis D E.Phys Rev,1992;45B:285
[11]Barth U Von,Hedin L.J Phys C:Solid State Phys,1972; 5:1615
[12]Chen L Q,Wang C Y,Yu T.Acta Phys Sin,2006;55: 5980 (陈丽群,王崇愚,于涛.物理学报,2006;55:5980)
[13]Chen L Q,Wang C Y,Yu Tao.J Appl Phys,2006;100: 023715
[14]Delley B.J Chem Phys,1990;92:508
[15]Delley B.J Chem Phys,1991;94:7245
[16]Wang C Y,Zhao D L.Mater Res Soc Symp Proc,1994; 318:571
[17]Wang C Y.Acta Metall Sin,1997;33:54 (王崇愚.金属学报,1997;33:54)
[18]Mulliken R S.J Chem Phys,1955;23:1833
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!