Please wait a minute...
Acta Metall Sin  2007, Vol. 42 Issue (1): 6-10     DOI:
Research Articles Current Issue | Archive | Adv Search |
Pore Distribution in Radial-type Regular Porous Structure
;
Cite this article: 

;. Pore Distribution in Radial-type Regular Porous Structure. Acta Metall Sin, 2007, 42(1): 6-10 .

Download:  PDF(216KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Regular porous metal with a radial pore distribution is produced by precipitation of supersaturated gas when the melt is bidirectionally solidified. A model was proposed to describe the ideal pore distribution of radial-type regular porous structure and rationality of the model was proved. This model can describe the effects of pore nucleation, pore coalition and pore interruption on structural characteristics and their quantitative relation can be deduced from the model. Probability of pore nucleation, pore coalition and pore interruption in the samples was also calculated.
Key words:  2D Gasar      Radial porous structure      Pore distribution      
Received:  30 May 2006     
ZTFLH:  TG249.6  
  TG146  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V42/I1/6

[1] Shapovalov V I.US Pat,5,181,549,1993
[2] Shapovalov V I.MRS Bull,1994;19(4):24
[3] Shapovalov V I,Boyko L.Adv Eng Mater,2004;6:407
[4] Hyun S K,Nakajima H.Mater Trans,2002;43:526
[5] Hyun S K,Nakajima H.Mater Lett,2003;57:3149
[6] Ikeda T,Aoki T,Nakajima H.Metall Mater Trans,2005; 36A:77
[7] Liu Y,Li Y X.Scr Mater,2003;49:379
[8] Liu Y,Li Y X,Wan J,Zhang H W.Mater Sci Eng,2005;A402:47
[9] Wang X, Li Y X, Liu Y. Acta Metall Sin, 2006; 42: 1075 (王雪,李言祥,刘源.金属学, 2006; 42: 1075)
[1] ZHUO Weijia, LIU Yuan, LI Yanxiang. EFFECT OF WITHDRAWING RATE ON PORE MORPHOLOGY OF LOTUS-TYPE POROUS COPPER PRODUCED BY SINGLE-MOLD GASAR TECHNIQUE[J]. 金属学报, 2014, 50(8): 921-929.
[2] . Effect of Transverse Convection Induced by Density Differences on Bidirectional Solidification of Metal-Gas Eutectic[J]. 金属学报, 2008, 44(9): 1057-1062 .
[3] Yuan Liu. Fabrication of Regular Porous Magnesium with Radial Pore Distribution[J]. 金属学报, 2006, 42(10): 1075-1080 .
[4] . [J]. 金属学报, 2005, 41(8): 886-890 .
[5] LIU Yuan; LI Yanxiang; ZHANG Huawei. FABRICATION OF LOTUS--STRUCTURED POROUS MAGNESIUM WITH GASAR PROCESS[J]. 金属学报, 2004, 40(11): 1121-1126 .
[6] . [J]. 金属学报, 2003, 39(7): 686-690 .
[7] . [J]. 金属学报, 2002, 38(7): 703-708 .
[8] . [J]. 金属学报, 2000, 36(2): 167-170 .
No Suggested Reading articles found!