Abstract The 3D deformation process of type-B PLC shearing band inAl-Cu alloy is captured by the help of a high speed digital photography with 1000 frames per second. A technique based on a novel high-speed digital speckle pattern metrology consisting of in-plane and out-of-plane deformation measurement methods is used for obtaining the playback of the 3D deformation process. The result shows one of the nucleation methods of type-B band: the shearing band initiates at a lateral specimen surface as a narrow band at an angle of 53 to the tensile axils and shears along the thickness direction. Subsequently the band front begins to propagate to the other lateral specimen surface along its length direction and expands in its width direction accompanying with the drop of the stress. When the front of the band reaches the other lateral surface, the band begins to expand in its width direction instantly and avalanchine shearing deformation happens. Based on the out-of-plane data, the relationship to the nucleation positions of following bands is that the latter one initiates on the front edge of the former one and the spacing of their center lines is half of the band width.
[1]Potevin A,Le Chatelier F.Compt Rend Acad Sci Paris,1923; 176:507 [2]Cottrell A H.Dislocation and Plastic Flow in Crystals.London:Oxford University Press,1953 [3]Lebyodkin M,Dunin-Barkowskii L,Brechet Y.Acta ??Mater,2004;8:2529 [4]Pink E,Weinhandl H.Scr Mater,1998;29:1309 [5]Tian B H,Zhang Y G,Chen C Q.Aeta Metall Sin,1996;32:249 (田宝辉,张永刚,陈昌麒.金属学报,1996;32:249) [6]Tian B H,Li H X,Zhang Y G,Chen C Q.Acta Metall Sin,1998;34:603 (田宝辉.李焕喜,张永刚.陈昌麒.金属学报,1998;34:603) [7]Chihab K,Estrin Y,Kubin L P.Scr Metall,1987;21:203 [8]Haehner P,Ziegenbein A,Rizzi E.Phys Rev,2002;65B:134109 [9]Wu X P,He S P,Li Z C.Acta Phys Sin,1983;32(8):1 (伍小平,何世平,李志超.物理学报,1983:32(8):1) [10]Jiang H F,Zhang Q C,Xu Y H,Wu X P.Acta Phys Sin,2006:55:409 (江慧丰,张青川,徐毅豪,伍小平.物理学报,2006;55:409) [11]Zhang Q C,Toyooka S,Wu X P.Proc SPIE,2002;4537:69 [12]Jiang Z Y,Zhang Q C,Wu X P.J Exp Mech,2003;18:289 (蒋震宇,张青川,伍小平.实验力学.2003;18:289) [13]Jiang Z Y,Zhang Q C,Jiang H F.Mater Sci Eng,2005;A403:154 [14]Zhang Q C,Zhen Y J,Jiang H F.Int J Plast,2005;21:2150 [15]Jiang H F,Zhang Q C,Zhen Y J.Chin Phys Lett,2005:22(1):99 [16]Tong W,Tao H,Zhang N.Scr Mater,2005;53:87 [17]Jiang H F,Zhang Q C,Jiang Z Y,Wu X P.Acta Metall Sin,2005;41:727 (江慧丰,张青川,蒋震宇,伍小平.金属学报,2005;41:727)