Effect of pre-compression on the stress rupture properties of single crystal superalloy:Ⅰmicrostructure and stress rupture properties of pre-compressed samples
中科院金属研究所
Cite this article: 

. Effect of pre-compression on the stress rupture properties of single crystal superalloy:Ⅰmicrostructure and stress rupture properties of pre-compressed samples. Acta Metall Sin, 2006, 42(8): 843-849 .

Download:  PDF(4507KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of uniaxial pre-compression on the microstructure and stress rupture properties of an second generation single crystal superalloy without Re is studied. The pre-compression is performed in vacuum at 1050℃ by 180MPa/6h and 220MPa/6h respectively. It is shown that P type γ’ paralleling to stress is formed during pre-compression, which is more regular in the 220MPa compressed sample. Moreover, dislocation networks are deposited on γ/γ’ interface in vertical channels, while a few dislocations have cut into γ’ particles in 220MPa compressed sample. The effect on stress rupture lifetime vary with the test conditions, but pre-compression increased the elongations under all test conditions.
Key words:       
Received:  21 November 2005     
ZTFLH:  TG146.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I8/843

[1]Pollock T M,Argon A S.Acta Metall Mater,1992;40:1
[2]Srinivasan R,Eggeler G F,Mills M J.Acta Mater,2000;48:4867
[3]Fredholm A,Strudel J L.In:Gell M,Kortvich C S,Bricknell R H,Kent W B,Radavich J F,eds.,Superalloys 1984,Warrendale,PA:AIME,1984:211
[4]Pollock T M,Argon A S.Acta Metall Mater,1994;42:1859
[5]Peng Z F,Feller-Kniepmeier M.Acta Metall Sin,1995;31:371 (彭志方,Feller-Kniepmeier M.金属学报,1995;31:371)
[6]Matan N,Cox D C,Rae C M F,Reed R C.Acta Mater,1999;47:2031
[7]Mughrabi H,Ott M,Tetzlaff U.Mater Sci Eng,1997;A234:434
[8]Tetzlaff U,Mughrabi H.In:Pollock T M,Kissinger R D,Bowman R R,Green K A,McLean M,Olson S L,Schirra J J,eds.,Superalloys 2000,Warrendale,PA:TMS,2000:273
[9]Nathal M,MacKay R,Miner R.Trans Metall,1989;20A:133
[10]Pearson D,Lemkey F,Kear B.In:Tien J K,Wlodek S T,MorrowⅢH,eds.,Superalloys 1980,Warrendale,PA:AIME,1980:513
[11]Schneider W,Hammer J,Mughrabi H.In:Antolovich S D,Stusrud R W,Mackay R A,Anton D L,Khan T,Kissinger R D,Klarstrom D L,eds.,Superalloys 1992,Warrendale,PA:TMS,1992:589
[12]Mughrabi H,Schneider W,Sass V,Lang C.In:Oikawa H,Maruyama K,Takeuchi S,Yamaguchi M,eds.,Proc 10th Int Conf Strength of Metals and Alloys,ICSMA 10,Sendai,Japan:Japan Institute of Metals,1994:705
[13]Veron M,Brechet Y,Louchet F.In:Kissinger R D,Nathal M V,Deye D J,Pollock T M,Anton D L,woodford D A,Cetel A D,eds.,Superalloys 1996,Warrendale,PA:TMS,1996:181
[14]Zhang J X,Wang J C,Harada H,Koizumi Y.Acta Mater,2005;53:4623
[15]Sherry A H,Pilkington R.Mater Sci Eng,1993;A172:51
[16]Liu J L,Jin T,Zhang J H,Hu Z Q.Acta Metall Sin,2001;37:1233(刘金来,金涛,张静华,胡壮麒.金属学报,2001;37:1233)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!