Abstract Effects of electric field annealing on plastic strain ratio (r value) of IF deep drawing steel sheet were studied by mean of tensile test. The results show that electric field annealing improves the average plastic strain ratio ( value). This is due to the fact that the electric field annealing reinforces the γ-fiber texture and weakens the a-fiber texture that deteriorated the plastic strain ratio.
|
|
Received: 01 December 2005
|
|
|
[1]Hutchinson W B.Int Met Rev,1982;27:307 [2]Urabe T,Jonas J J.ISIJ Int,1994;34:435 [3]Ray R K,Jonas J J,Hook R E.Int Met Rev,1994;39:129 [4]Conrad H,Karam N,Mannan S.Scr Metall,1983;17:411 [5]Lu H A,Conrad H.Appl Phys Lett,1991;59:47 [6]Conrad H,Guo Z,Sprecher A F.Scr Metall,1989;23:821 [7]Li M Q,Wu S.Scr Metall Mater,1994;31:75 [8]Liu W,Liang K M,Zheng Y K,Cui J Z.Scr Mater,1996;15:1327 [9]He C S,Zhang Y D,Wang Y N,Zhao X,Zuo L,Esling C.Scr Mater,2003;48:737 [10]Whiteley R L.Trans ASM,1960;52:154 [11]Schulz L G.J Appl Phys,1949;20:1030 [12]Liang Z D,Xu J Z,Wang F.Three Dimensional Orientation Distribution Analysis of Textured Materials—ODF Analysis.Shenyang:Northeast University of Technology Press,1986:108 (梁志德,徐家祯,王福.织构材料的三维取向分析术—ODF分析.沈阳:东北工学院出版社,1986:108) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|