Please wait a minute...
Acta Metall Sin  2006, Vol. 42 Issue (2): 118-122     DOI:
Research Articles Current Issue | Archive | Adv Search |
Constrain of Alternating Stress Field on Glide Dislocations in Cu/Ni Multilayers
大连海事大学轮机工程学院
Cite this article: 

. Constrain of Alternating Stress Field on Glide Dislocations in Cu/Ni Multilayers. Acta Metall Sin, 2006, 42(2): 118-122 .

Download:  PDF(464KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  29 April 2005     
ZTFLH:  TB43  
  O346.3  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I2/118

[1] Lloyd S J, Molina-Aldareguia J M. Philos Trans R Soc Lond, 2003; 361A: 2931
[2] Misra A, Kung H, Embury J D. Scr Mater, 2004; 50: 707
[3] Paldey S, Deevi S C. Mater Sci Eng, 2003; A342: 58
[4] Was G S, Foecke T. Thin Solid Films, 1996; 286: 1
[5] Yashar P, Sproul W D. Vacuum, 1999; 55: 179
[6] Zhang S, Sun D, Fu Y Q, Du H J. Surf Coat Technol, 2003; 167: 113
[7] Koehler J S. Phys Rev, 1970; B2: 547
[8] Lehoczky S L. J Appl Phys, 1978; 49: 5479
[9] Anderson P M. Scr Metall Mater, 1992; 27: 687
[10] Embury J D, Hirth J P. Acta Metall Mater, 1994; 42: 2051
[11] Hall E O. Proc Phys Soc, 1952; B64: 747
[12] Petch N J. J Iron Steel Inst, 1953; 174: 25
[13] Wadley H N G, Zhou X W, Johnson R A, Neurock M. Prog Mater Sci, 2001; 46: 329
[14] Zhou X W, Wadley H N G, Johnson R A. Acta Mater, 2001; 49: 4005
[15] Alber I, Bassani J L, Khantha M, Vitek V, Wang G J. Philos Trans R Soc Lond, 1992; 339A: 555
[16] Cheng D, Yan L, Yan Z J. Thin Solid Films, in press
[17] Cheng D, Yan L, Yan Z J. J Fund Mater, 2005; 36: 918 (程东,严立,严志军.功能材料,2005;36:918)
[18] Zhou X W, Johnson R A, Wadley H N G. Ada Mater, 1997; 45: 1513
[19] Barshilia H C, Rajam K S. Surf Coat Technol, 2002; 155: 195s
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!