| Fabrication of Regular Porous Magnesium with Radial Pore Distribution |
| Yuan Liu |
| 清华大学机械工程系材料加工技术研究所 |
|
Cite this article:
Yuan Liu. Fabrication of Regular Porous Magnesium with Radial Pore Distribution. Acta Metall Sin, 2006, 42(10): 1075-1080 .
|
|
|
Abstract By use of the Gasar process (unidirectional solidification of metal-gas eutectic), porous magnesium samples with radial pore distribution have been fabricated successfully through altering the heat transferring from the axial to radial direction. In addition, this paper also studied the structural features and the effect of gas pressure on porosity, pore size and distribution.
|
|
Received: 12 September 2005
|
|
|
[1]Shapovalov V I.US Pat,No.5,181,549,1993 [2]Shapovalov V I,Boyko L.Adv Eng Mater,2004;(6):407 [3]Nakajima H,Hyun S K,Ohashi K.Colloid Surf,2001;179A:209 [4]Hyun S K,Nakajima H.Mater Trans,2002;43:526 [5]Hyun S K,Nakajima H.Mater Lett,2003;57:3149 [6]Ikeda T,Aoki T,Nakajima H.Metall Mater Trans,2005;36A:77 [7]Liu Y,Li Y X,Zhang H W,Wan J.Acta Metall Sin,2005;41:886 ??(刘源,李言祥,张华伟,万疆.金属学报,2005;41:886) [8]Liu Y,Li Y X,Zhang H W.Acta Metall Sin,2004;40:1121(刘源,李言祥,张华伟.金属学报,2004;40:1121) [9]Liu Y,Li Y X,Zhang H W.Rare Met Mater Eng,2005;34:1128(刘源,李言祥,张华伟.稀有金属材料与工程,2005;34:1128) [10]Liu Y,Li Y X,Wan J,Zhang H W.Mater Sci Eng,2005;A402:47 [11]Manchester F D.Phase Diagrams of Binary Hydrogen Alloys.Materials Park,Ohio:ASM International,2000:83 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|