| Intermediate Transformation Structures in a Low Carbon Mo--Cu--Nb--B Microalloying Steel |
| ZHAO Yuntang; SHANG Chengjia; HE Xinlai; GUO Hui |
| School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
ZHAO Yuntang; SHANG Chengjia; HE Xinlai; GUO Hui. Intermediate Transformation Structures in a Low Carbon Mo--Cu--Nb--B Microalloying Steel. Acta Metall Sin, 2006, 42(1): 54-58 .
[1]Ohtani H,Okaguchi S,Fujishro Y,Ohmori Y.Metall Trans,1990;21A:877 [2]Krauss G,Thomposon T W.ISIJ Int,1995;35:937 [3]Bhadeshia H K D H,Svensson L E.J Mater Sci,1989;24:3180 [4]All A,Bhadeshia H K D H.Mater Sci Technol,1991;7:895 [5]Shang C J,Wang X M,Yang S W,He X L,Wu H B.Acta Metall Sin,2003;39:1019(尚成嘉,王学敏,杨善武,贺信莱,武会宾.金属学报,2003;39:1019) [6]Shang C J,Hu L J,Yang S W,Wang X M,Zhao Y T,He X L.Aeta Metall Sin,2005;41:471(尚成嘉,胡良均,杨善武,王学敏,赵运堂,贺信莱.金属学报,2005;41:471) [7]Bhadeshia H K D H.Bainite in Steels(2nd ed).Cambridge:The Cambridge University Press,2001 [8]Thompson S W,Colvin D J,Krass G.Metall Trans,1990;21A:1493 [9]Rodrigues P C M,Pereloma E V,Santos D B.Mater Sci Eng,2000;A283:136 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|