| Effect of Dynamic Precipitation on Creep Behavior of Mg—5Zn—2Al(--2Y) Alloy |
| ZOU Honghui; ZENG Xiaoqin; ZHAI Chunquan; DING Wenjiang |
| State Key Laboratory of Metal Matrix Composite; Shanghai Jiaotong University; Shanghai 200030 |
|
Cite this article:
ZOU Honghui; ZENG Xiaoqin; ZHAI Chunquan; DING Wenjiang. Effect of Dynamic Precipitation on Creep Behavior of Mg—5Zn—2Al(--2Y) Alloy. Acta Metall Sin, 2006, 42(1): 41-48 .
[1]cáceres C H,Rovera D M.J Light Met,2001;1:151 [2]Arne K D,Young C L,Mark D N,Pollock T M.J Light Met,2001;1:61 [3]Moreno I P,Nandy T K,Jones J W,Allison J E.Scr Mater,2003;48:1029 [4]Polmear I.J Mater Trans JIM,1996;1:12 [5]Lou C P,Xiao X L,Liu J W.Acta Metall Sin,2001;38:709(罗承萍,肖晓玲,刘江文.金属学报,2002;38:709) [6]Zhang Z,Couture A,Luo A.Scr Mater,1998;39:45 [7]Wei L Y,Dunlop G L,Westengen H.Metall Mater Trans,1995;26A:1947 [8]Guo T W,Li A D,Xu J P.Theories of the High Temperature Strength and Design of Metal Materials.Beijing:Science Press,1983:51(郭廷玮,李安定,徐介平.金属材料的高温强度理论·设计.北京:科学出版社,1983:51) [9]Sunhak L,Seung L,Do Hyang K.Metall Mater Trans,1998;29A:1221 [10]Wei L Y,Dunlop G L J.Alloys Compd,1996;232:264 [11]Kim S H,Kim D H,Kim N J.Mater Sci Eng,1997;A226,1030 [12]Nie J F.Scr Mater,2003;48:1009 [13]Nie J F,Muddle B C.J Phase Equilibria,1998;19:543 [14]Mili(?)ka K,(?)adeK J,Rys P.Acta Metall,1970;18:1071 [15]Hirth J P,Lothe J.Theory of Dislocations.New York:McGraw-Hill Book Company,1982:57 [16]Regev M,Rosen A,Bamberger M.Metall Mater Trans,2001;32A:1335 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|