| Stabilization of Austenite in Quenched Alloy Steels |
| KANG Mokuang; ZHU Ming |
| School of Materials; Northwestern Polytechnical University; Xi'an 710072 |
|
Cite this article:
KANG Mokuang; ZHU Ming. Stabilization of Austenite in Quenched Alloy Steels. Acta Metall Sin, 2005, 41(7): 673-679 .
|
|
|
Abstract
Retained austenite exists in alloy steels both continuously
quenched and isothermally quenched, so its content relates to the austenitic
stabilization. The article focuses on the investigation for the austenitic
stabilization in isothermally quenched microstructures from duplex phase
(martensite--M, bainite--B) temperature region. Within a certain
isothermal time, the relationship of the amount of retained
austenite AR vs isothermal
temperature is a saddle--like curve, and the valley
value for testing steel is less than that of continuous
quenching with a same cooling medium, which proves
that isothermal soak does not increase retained
austenitic quantity on certain condition. By adjusting
the content ratios of AR/M and AR/B on
the saddle--like curve, an isothermal quenching of the
less deformation or a meta-bainitic isothermal quenching
with strength--toughness optimized combination
can be achieved. Austenitic stabilization is the synthetic
effect of thermal, chemical, phase induced and macro--thermal
stress stabilized mechanisms. The martensite
critical point Mc has not
the special physical meaning.
|
|
Received: 24 October 2004
|
|
|
[1] Cubberly W H, Masseria V, Kirpatrik C W, Sanders B. Metals Handbook, (Vol.4), 9ed. Metals Park Ohio: American Society Metals, 1981: 117, 599 [2] Zackay V F, Paker E R, Fahr D, Bush R. Trans Soc Metall, 1967; 60: 252 [3] Matsumura O, Sakuma Y, Takechi H. Trans ISIJ, 1987; 27: 570 [4] Webster D. Metall Trans, 1971; 2A: 1857 [5] Lou B, Averbach B L. Metall Trans, 1983; 14A: 1899 [6] Paker E R, Zackay V F. Eng Fract Mech, 1975; 7: 371 [7] Gregary H. Steel Res, 1995; 66: 433 [8] Wen C, Lin J, Zhou Y. Ada Metall Sin (Engl Lett), 1996; 9: 59 [9] Bhadeshia H K D H, Edmonds D V. Met Sci, 1983; 17: 420 [10] Liu D Y, Fang H S, Bai B Z. Trans Mater Heat Treat, 2002; 23(4): 57 (刘东雨,方鸿生,白秉哲.材料热处理学报,2002;23(4):57) [11] Mathaws J A. Trans Soc Steel Treat, 1925; 8: 565 [12] Morgen E A, Ko T. Acta Metall, 1953; 1: 36 [13] Holloman J H. J Appl Phys, 1947; 18: 1421 [14] Cohen M. Trans ASM, 1949; 41: 35 [15] Xu Z Y. Martensitic Transformation and Martensite. Beijing: Science Press, 1980: 56, 61 (徐祖耀.马氏体相变与马氏体.北京:科学出版社,1980:56, 61) [16] Haidemenopouls G N, Vasilakos A N. J Alloys Gompd, 1997; 247: 128 [17] Mohahcy O N. Mater Sci Eng, 1995; B32: 267 [18] Kang M K, Yang S P, Guan D H. Bainite in Steels. Shanghai: Shanghai Science Press, 1990: 190, 208, 282, 376 (康沫狂,杨思品,管敦惠.钢中贝氏体.上海:上海科技出版 社, 1990:190,208,282,376) [19] Ko T. JISI, 1953; 175: 36 [20] Kang M K, Sun J L, Yang Q M. Metall Trans, 1990; 21A: 853 [21] Lifshiz V G. Physical Properties of Metals and Their Alloys, Russian Maskva, 1956 [22] Harries W, Cohen M. Met Technol, 1948; No.2446: 21 [23] Kang M K. Proc of First Conf of Heat Treatment Institution of EMES, Beijing: China Machine Press, 1966: 96 (康沫狂.中国机械工程学会热处理学会第一届年会论文集,北 京:机械工业出版社,1966:96) [24] Blanjer M E. Phase Transformation for Heat Treatment of Steels. Russian: Metallurgical Press, 1962: 121 [25] Thomas G, Sarikaya M. In: Proc Inter Conf of Solid-Solid Phase Transformations, New York: TMS-AIME, 1982: 999 [26] Huang D H, Thomas G. Metall Trans, 1971; 2A: 1587 [27] Friedel J. Dislocations, Paris: Pergomon Press, 1964: 270 [28] Clark R, Thomsa G. Metall Trans, 1975; 5: 699 [29] Rao B V N, Thomsa G. Metall Trans, 1980; 11A: 441 [30] Kang M K, Zhu M. Heat Treat Met, 2005; 31(1): 14 (康沫狂,朱明.金属热处理,2005;31(1):14) [31] Xu Z Y. Shanghai Met, 1982; 4(4): 46 (徐祖耀.上海金属,1982;4(4):46) [32] Magee C L. Phase Transformations, Metals Park, Ohio: ASM, 1970; 115 [33] Lee Y K, Shn H C, Jang Y C,Kim S H, Chai C S. Scr Mater, 2002; 47: 805 [34] Patel J R, Cohen M. Acta Metall, 1953; 1: 531 [35] Xu Z Y. Acta Metall Sin, 2004; 40: 113 (徐祖耀.金属学报,2004;40:113) [36] Denis S, Gaatier E, Simon A, Beek G. Mater Sci Technol, 1985; 1: 805 [37] Yong J R, Huang C Y, Hsieh W H, Chiou C S. Mater Trans JIM, 1996; 37: 579 [38] Nahimov D M. Handbook (Metallography and Heat Treatment of Steels and Cast Irons), Russian: Metallurgical Press, 1956: 380 |