| Inverse Algorithm of Heat Transfer in Round Billet Continuous Casting Mould |
| YIN Hebi; YAO Man |
| Department of Materials Engineering ; Dalian University of Technology; Dalian 116023 |
|
Cite this article:
YIN Hebi; YAO Man. Inverse Algorithm of Heat Transfer in Round Billet Continuous Casting Mould. Acta Metall Sin, 2005, 41(6): 638-644 .
|
|
|
Abstract Based on the measured data of mould temperatures during continuous
casting of round billet, an inverse problem model was developed.
Through identifying the local thermal resistance and its distribution
between the mould and the strand, the mould heat flux and the shell
thickness profiles were calculated, and the relationship between them
was also analyzed. The calculated results could preciously and correctly
reflect the characteristics of non-uniform heat transfer around
the mould circumference, which provided an applicable method for
applying numerical simulation technique to monitor the
solidification process and the“visual mould”technology in
continuous casting.
|
|
Received: 31 August 2004
|
|
|
[1]Brimacombe J K.Metall Trans,1993;24B:917 [2]Bakshi I A,Brendzy J L,Walker B N,Chandra S,Sama- rasekera I V,Brimacombe J K.Ironmaking Steelmaking, 1993;20:54 [3]Emling W H,Dawson S.ISS 74th Steelmaking Conf Proc, Washington,DC:Iron and Steel Society of AIME,1991: 197 [4]Lang O,Federspiel C,Thalhammer M,Watzinger J.Steel World,2000;5:38 [5]Zhang J M,Zhang L,Wang X H,Wang L F.Ada.Metall Sin,2003;39:1285 (张炯明,张立,王新华,王立峰.金属学报,2003;39:1285) [6]Zhang X Z,Na X Z,Wang Z Y,Liu A Q,Gan Y.Acta Metall Sin,2004;40:281 (张兴中,那贤昭,王忠英,刘爱强,干勇.金属学报,2004;40:281) [7]Liu X,Yin H B.In:Li W X,ed.,CSM 2003 Annual Meeting Proc,Beijing:Metallurgical Industry Press,2003:413 (刘晓,尹合壁.见:李文秀主编,2003年中国钢铁年会论文集,北京:冶金工业出版社,2003:413) [8]Sun J,Pan D H.Res Iron Steel,1998;(5):21 (孙冀,潘德惠.钢铁研究,1998;(5):21) [9]Pinheiro C A M,Samarasekera I V,Brimacombe J K,Walker B N.Ironmaking Steelmaking,2000;27:37 [10]Huespe A E,Cardona A,Fachinotti V.Comput Methods Appl Mech Eng,2000;182:439 [11]Mahapatra R B,Brimacombe J K,Samarasekera I V.Metall Trans,1991;22B:875 [12]Mills K C,Fox A B.ISIJ Int,2003;43:1479 [13]Billany T J H,Normanton A S,Mills K C,Grieveson P.Ironmaking Steelmaking,1991;18:403 [14]Irving W R,Perkins A.Ironmaking Steelmaking,1977;4:292 [15]Ikeda M,Asano K,Nakano T,Fuji M,Mizoguchi S,Misumi H.Trans Iron Steel Inst Jpn,1981;21:B511 [16]Sugitani Y,Nakamura M,Okuda M,Kawasaki M,Naka-jima K.Trans Iron Steel Inst Jpn,1985;25:B91 [17]Mills K C,Billany T J H,Normanton A S,Walker B N,Grieveson P.Ironmaking Steelmaking,1991;18:253= |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|