| The analysis of periodic layer formation during solid state reactions |
| CHEN Yongchong; QI Lu; ZHANG Yonggang; CHEN Changqi |
| College of Chemistry & Molecular Engineering; Peking University; Beijing 100871 |
|
Cite this article:
CHEN Yongchong; QI Lu; ZHANG Yonggang; CHEN Changqi. The analysis of periodic layer formation during solid state reactions. Acta Metall Sin, 2005, 41(3): 235-241 .
|
|
|
Abstract As one of the most interesting diffusion phenomena discovered
by Osinski et al. in 1982, the periodic layer formation
during solid state reactions is still far from a satisfactory
description. Since the successive layers have facing
surfaces with mated topography, it is
considered that the seperating of the layer from the reaction
front should relate to the diffusion-induced
stresses developing within the separating of the layer during
solid state reactions. We discovered that the layer is
fractal with clusters of phase β(FeSi in
diffusion couple Zn/Fe3Si or CoSi in diffusion couple
Zn/Co2Si, e.g.) distributing continuously in phase α
(FeZn13 or CoZn13, respectively). This
empirical fact supports the mechanical-instability
model for the pattern formation of
periodic-layered structures.
|
|
Received: 29 April 2004
|
|
|
[1] Osinski K, Vriend A W, Bastin G F, van Loo F J J. Z Metallkd, 1982; 73: 258 [2] van Loo F J J, Osinski K. In: Purdy G R ed., Fundamentals and Applications of Ternary Diffusion. Oxford: Pergamon Press, 1990: 109 [3] Dunaev S F, Zver'kov S A. J Less-Common Met, 1989; 153: 143 [4] Chou T C. J Mater Res, 1990; 5: 601 [5] Kao C R, Chang Y A. Acta Metall Mater, 1993; 41: 3463 [6] Rijnders M R, Kodentsov A A, Cserhati C S, van den Akker J, van Loo F J J. Defect Diffus Forum, 1996; 129-130: 253 [7] Greer A L. Defect Diffus Forum, 1996; 129-130: 339 [8] Kuo K. Iron Steel Inst London, 1954; 176: 433 [9] Fridberg J, Hillert M. Acta Metall, 1977; 25: 19 [10] Howell P R. Mater Charact, 1998; 40: 227 [11] Kodentsov A A, Rijnders M R, van Loo F J J. Acta Mater, 1998; 46: 6521 [12] Kodentsov A A, van Dal M J H, Cserhati C, Gusak A M, van Loo F J J. Defect Diffus Forum, 2001; 194-199: 1491 [13] Chen Y C, Zhang Y G, Chen C Q. Mater Sci Eng, 2003; A362: 135 [14] Chen Y C, Zhang Y G, Chen C Q. Mater Sci Eng, 2004; A368: 1% |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|