Please wait a minute...
Acta Metall Sin  2004, Vol. 40 Issue (8): 887-890     DOI:
Research Articles Current Issue | Archive | Adv Search |
EFFECTS OF HEAT TREATMENT TEMPERATURE ON MICROSTRUCTURE AND PROPERTIES OF WIRE--DRAWN Cu--12Ag FILAMENTARY COMPOSITE
Cite this article: 

. EFFECTS OF HEAT TREATMENT TEMPERATURE ON MICROSTRUCTURE AND PROPERTIES OF WIRE--DRAWN Cu--12Ag FILAMENTARY COMPOSITE. Acta Metall Sin, 2004, 40(8): 887-890 .

Download:  PDF(707KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  01 January 1900     
ZTFLH:  TB331  
  TG146.3  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I8/887

[1] Yoshitaka A. In: Enomoto M ed., New Structure Steels and New Design of Constructions, 6th Workshop on the Ultra-steel, Tsukuba: The Iron and Steel Institute of Japan, 2002: 91
[2] Adachi Y, Tomida T, Hinotani S. ISIJ, 2003; 40: S194
[3] Rainforth W M, Black M P, Higginson R L, Palmiere E J. Acta Mater, 2002; 50: 735
[4] Lai Z H. Crystal Defects and Mechanical Properties of Metals, Beijing: Metallurgy Industry Press, 1988: 294(赖祖涵,金属的晶体缺陷与力学性能,北京:冶金工业出版社,1988:294)
[5] Yang S W, Shang C J, Wang X M, He X L. J Univ SciTechnol Beijing, 2001; 3: 214
[6] Yang S W, He X L, Chen M Z, Dang Z J, Ke J. Mater SciEng, 1994; 2: 49(杨善武,贺信莱,陈梦谪,党紫九,柯梭,材料科学与工程,1994;2:49)
[7] Feng D. Physics of Metals, Vol.1, Beijing: Science Press, 2000: 266(冯端,金属物理学,第一卷,北京,科学出版社,2000:266)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!