    					| Synthesis of W--20%Cu Nanocomposite Powders | 
  					 
  					  										
						| YANG Mingchuan; SONG Zhenzhen; LU Ke | 
					 
															
						| Shenyang National Laboratory for Materials Science; Institute of Metal Research; The ChineseAcademy of Sciences; Shenyang 110016 | 
					 
										
						 | 
					 
				 
				
				Cite this article: 
				
					
			      YANG Mingchuan; SONG Zhenzhen; LU Ke. Synthesis of W--20%Cu Nanocomposite Powders. Acta Metall Sin, 2004, 40(6): 639-.	
				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
              
				
												  
													
													    | 
													    	
														 | 
													 
																										
													
														| 
															
													     		                            						                            																	    Abstract  W--20%Cu (mass fraction) nanocomposite powders were synthesized by means of combining spray drying and hydrogen reduction process. The composite powders were characterized by using XRD, SEM, TEM. It has been shown that tungsten and copper are homogenously mixed within each particle and the average particle size is about 240 nm, in which the tungsten particles have an average grain size of 16 nm.
																										     | 
														 
												  		
														
															| 
															    																	Received:  17 March 2003
																	    
															    															    															  
															 | 
															
														 
														 														
															| 
																
															 | 
														 
																																									    																											 
												 
												
												
												
												 
												
												  
             
                         
            
									            
									               
																												  
															  [1] Cai Y X, Liu B W. Powder Metall Technol, 1999; 17(2) :138(蔡一湘,刘伯武.粉末冶金技术,1999;17(2) :138)  [2] Liv D M. Powder Metall Ind, 1998: 8(6) : 32(吕大铭.粉末冶金工业,1998;8(6) :32)  [3] Sebastian K V. Int J Powder Metall Powder Technol,1981; 17: 297 [4] Neumann W, Kny E. High Temp High Press, 1989; 21:525 [5] Liv D M. Chin Tungsten Ind, 1999; 14(5/6) : 182(吕大铭.中国钨业,1999;14(5/6) :182)  [6] Jia C C, Jin X H, Zhao J, Xie Z Z. Powder Metall Technol,2001; 19(3) : 148(贾成厂,金雪华,赵军,解子章.粉末冶金技术,2001;19(3) :148)  [7] Huang J Z, Li J Y, Wang J Y. Rare Met Cem Carbides,1989; 6: 67(黄建忠,李晋尧,王建业.稀有金属与硬质合金、1989;6:67)  [8] Johnson J L, German R M. Metall Trans A, 1993;(24A):2369 [9] Moon I H, Lee J S. Powder Metall, 1979; 22: 5 [10] Moon I H, Lee J S. Powder Metall Int, 1977; 9: 23 [11] Kirk T W, Caldwell S G, Oakes J J. Adv Powder Metall Particulate Materials--1992, Princeton. NJ: MPIF, 1992;9: 115 [12] Tao Y Q, Wang Z P, Fang N X, Wu Z C. Powder Metall Technol, 2002; 20(1) : 49(陶应启,王祖平,方宁象,吴仲春.粉末冶金技术,2002;20(1) :49)  [13] Chen W G, Ding B J. Powder Metall Ind, 2001; 11(3) : 45(陈文革,丁秉均.粉末冶金工业;2001;11(3) :45)  [14] Cannon H S, Lenel F V. In: Benesovsky F ed, Proc 1st Plansee Seminar, Reutte, Austria: Metallwerk Plansee,1953: 106 [15] Benjamin J S. Met Trans, 1970; 8(1) : 2943 [16] McCandlish L E, Kear B H, Kim B K. Nanostructured Mater, 1992; 1: 119 [17] Chen Q L, Tang C Q, Xiao X. Mater Sci Eng, 2002; 20:224(陈琦丽,唐超群,肖循.材料科学与工程,2002;20:224)  [18] Chang W, Skandan G, Danforth S C, Kear B H, Hahn H.Nanostructured Mater,1994; 4/5: 507 [19] Birringer R, Gleiter H, Klein P H. Phys Lett A, 1984; 102:365 | 
														   
																											 
									             
									           
             
			            			 
			
             
								                
															
																
																	
																																																																									
																				| No Suggested Reading articles found! | 
																			 
																																			 
																 | 
															 
														 
								             
             
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |