Effect of Sodium Salicylate on Electropolymerization of Pyrrole on Zincated Steel
YIN Renhe; ZHAO Yaping;DAI Yingchun; ZHANG Xinsheng
Department of Chemistry; College of Science; Shanghai University; Shanghai 200436;National United Chemical Engineering Laboratory; East China University of Science and Technology; Shanghai 200237
Cite this article: 

YIN Renhe; ZHAO Yaping; DAI Yingchun; ZHANG Xinsheng. Effect of Sodium Salicylate on Electropolymerization of Pyrrole on Zincated Steel. Acta Metall Sin, 2004, 40(2): 168-172 .

Download:  PDF(3961KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The role of sodium salicylate in electropolymerization of pyrrole on zincated steel was studied by cyclic voltammetry. The results show that as supporting electrolyte, the sodium salicylate inhibits the zinc dissolution and favours the electropolymerization of pyrrole by passivating the substrate. Consequently, an uniform and compact polypyrrole film may be formed on zincated steel.
Key words:  sodium salicylate      electropolymerization      cyclic voltammetry      
Received:  28 January 2003     
ZTFLH:  TG174.2  
  TG178  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I2/168

[1] Ferreira C A, Aeiyach S, Aaron J J, Lacaze P C. Electrochim Acta, 1996; 41: 1801
[2] Hlser P, Beck F. J Appl Electrochem, 1990; 20: 596
[3] Warren L F, Anderson D P. J Electrochem Soc, 1987; 134: 101
[4] Hermelin E, Petitjean J, Aeiyach S, Lacroix J C, Lacaze P C. J Appl Electrochem, 2001; 31: 905
[5] Gu SY. Mater Protect, 2000; 33(4) : 41(顾书英.材料保护,2000;33(4) :41)
[6] Zheng Y B, Zhang S J, Ke Y C, Wu Z W. J Funct Polym, 1996; 9: 613(郑玉斌,张善举,柯杨船,吴忠文.功能高分子学报,1996:9:613)
[7] Li C G, Cui G, Yin S L, Jiang G Z. Chin J Anal Chem, 1994; 22: 922(李春光,崔刚,尹寿立,姜光哲.分析化学,1994;22:922)
[8] Xiao S T, Xu J, Huang Y, Li L. J South Chin Univ Technol (Nat Sci), 1998; 26(1) : 95(肖诗铁,徐俊,黄怡,李炼.华南理工大学学报(自然科学版),1998;26(1) :95)
[9] Wei P H, Liang W, Wang Y J. J Shandong Educ Coll, 2002; 17(1) : 84(魏培海,梁玮,王娅娟.山东教育学院学报,2002;17(1) :84)
[10] Petitjean J, Aeiyach S, Lacroix J C, Lacaze P C. J Electroanal Chem, 1999; 478: 92
[11] Liu Y H. Electrochemical Techniques. Beijing: Beijing Aeronautics College Press, 1987: 136(刘永辉.电化学测试技术.北京:北京航空学院出版社,1987:136)
[12] Silverstein R M, Webster F X. Spectrometric Identification of Organic Compounds: 6th ed., New York: John Wiley & Sons, 1998
[13] Zhou M, Heinze J. Electrochim Acta, 1999; 44: 1733
[14] Gilani T H, Ishiguro T. Synth Met, 1997; 84: 845
[15] Garcia B, Blanger D. Synth Met, 1998; 98: 135
[1] YANG Yulin, MU Zhangyan, FAN Zheng, DAN Zhenhua, WANG Ying, CHANG Hui. Nanoporous Silver via Electrochemical Dealloying and Its Superior Detection Sensitivity to Formaldehyde[J]. 金属学报, 2019, 55(10): 1302-1310.
[2] SONG Lixiao ZHANG Zhao ZHANG Jianqing CAO Chunan. ELECTROPLATING MECHANISM OF NANOSTRUCTURED BLACK Ni FILMS[J]. 金属学报, 2011, 47(1): 123-128.
[3] SHI Jinjie SUN Wei GENG Guoqing. INFLUENCE OF CARBONATION ON THE CORROSION PERFORMANCE OF STEEL HRB335 IN SIMULATED CONCRETE PORE SOLUTION[J]. 金属学报, 2011, 47(1): 17-24.
[4] ;. EXPERIMENTAL RESEARCH OF PREPARATION OF CaB6 BY MOLTEN SALT ELECTROLYSIS METHOD[J]. 金属学报, 2008, 44(10): 1243-1246 .
[5] DU Senlin;SU Mingzhong;Changchun Institute of Applied Chemistry; Academia Sinica. ELECTROCHEMICAL BEHAVIOUR OF Nd~3+ REDUCED ON LIQUID Ga ELECTRODE IN MOLTEN CHLORIDE[J]. 金属学报, 1991, 27(3): 111-115.
No Suggested Reading articles found!