| Effect of Initial Grain Size on Dynamic Recrystallization of Ferrite in |
| LI Longfei; YANG Wangyue;SUN Zuqing |
| School of Materials Science & Engineering; University of Science |
|
Cite this article:
LI Longfei; YANG Wangyue; SUN Zuqing. Effect of Initial Grain Size on Dynamic Recrystallization of Ferrite in. Acta Metall Sin, 2004, 40(2): 141-147 .
|
|
|
Abstract The hot deformation behavior and the microstructure evolution of a low
carbon steel with different initial grain sizes are investigated by
uniaxial hot compression at deformation temperatures of 700 ℃ and 600 ℃
and strain rates of 10 s-1 to 10-3 s-1.
The effect of initial grain size and hot deformation parameter Z on
dynamic recrystallization of ferrite is approached. The results indicate
that under the present deformation conditions, the dynamic
recrystallization of ferrite takes place in the low carbon steel. The
decrease of initial grain size is not only of benefit to the dynamic
recrystallization of ferrite at a certain Z value, but also leads to
the increase of the critical values of Z for both the dynamic
recrystallization of ferrite and the discontinuous dynamic recrystallization
of ferrite. It is suggested that the fine ferrite formed by deformation
enhanced transformation is beneficial to the occurrence of dynamic
recrystallization of ferrite during hot deformation. Further refinement
of the fine ferrite can be realized by the dynamic
recrystallization of ferrite under a suitable Z value.
|
|
Received: 24 February 2003
|
|
|
[1] Sun Z Q, Yang W Y, Qi J J, Hu A M. Mater Sci Eng, 2002; 334A: 201 [2] Sakai T, Jonas J J. Acta Metall, 1984; 32: 189 [3] Li L F, Yang W Y, Sun Z Q. Acta Metall Sin, 2003; 39: 419(李龙飞,杨王玥,孙祖庆.金属学报, 2003; 39: 419) [4] Yang W Y, Wang H M, Li L F, Sun Z Q. Acta Metall Sin, 2003; 39: 691(杨王玥,王红梅,李龙飞,孙祖庆.金属学报,2003;39:691) [5] Glover G, Sellars C M. Metall Trans, 1973; 4: 765 [6] Tsuji N, Matsubara Y, Saito Y. Scr Mater, 1997; 37: 477 [7] Tsuji N, Matsubara Y, Saito Y, Maki T. J Jpn Inst Met, 1998; 62: 967((?)伸泰,松原行宏,斋藤好弘,牧正志.日本金属学会志,1998;62:967) [8] Gao F, Xu Y, Song B, Xia K. Metall Mater Trans, 2000; 31A: 21 [9] Li L F, Yang W Y, Sun Z Q, Wang Q F. J Univ Sci Technol Beijing, 2001; 23: 225(李龙飞,杨王玥,孙祖庆,王青峰.北京科技大学学报,2001;23:225) |