| MAGNETIC PROPERTIES AND GIANT MAGNETOIM-PEDANCE EFFECT IN AS DEPOSITED (Fe88Zr7B5)0.97Cu0.03 FILMS |
| CHEN Weiping;XIAO Shuqin; WANG Wenjing; LIU Yihua |
| Department of Physics; Zhejiang Taizhou College; Linhai 317000 |
|
Cite this article:
CHEN Weiping; XIAO Shuqin; WANG Wenjing; LIU Yihua. MAGNETIC PROPERTIES AND GIANT MAGNETOIM-PEDANCE EFFECT IN AS DEPOSITED (Fe88Zr7B5)0.97Cu0.03 FILMS. Acta Metall Sin, 2004, 40(12): 1295-1298 .
|
|
|
Abstract The soft magnetic properties and giant magnetoimpedance (GMI) effect of the
amorphous films of Fe88Zr7B5 and
(Fe88Zr7B5)0.97Cu0.03 prepared by radio frequency
sputtering on the substrate of single crystal Si have been measured.
Significant results obtained is that the GMI effect almost can not be
detected in the as-deposited Fe88Zr7B5 films, while it
becomes evident for as-deposited
(Fe88Zr7B5) 0.97Cu0.03 films. The maximum values
of longitudinal and transverse GMI ratio are 17% and 11% at the frequency
of 13 MHz, respectively, indicating that the amorphous
(Fe88Zr7B5) 0.97Cu0.03 films have good soft magnetic
properties and GMI effect even though in the as-deposited state.
|
|
Received: 06 January 2004
|
|
|
[1] Mohri K, Kohzawa T, Kawashima K, Yoshida H, PaninaL V. IEEE Trans Magn, 1992; 28: 3150 [2] Suzuki K, Makino A, Inoue A, Masumoto T. J Appl Phys,1993; 74: 3316 [3] Kojima A, Makino A, Kawamura Y, Inoue A, MasumotoT. J Appl Phys, 1996; 35: L19 [4] Suzuki K, Makino A, Inoue A, Masumoto T. J Appl Phys,1993; 70: 6232 [5] Chen C, Zhao T Y, Guo H Q, Mei L M, Liu Y H, Shen BG, Zhao J G. J Phys Condens Matter, 1997; 9: 1951 [6] Aragoneses P, Holzer D, Sassik H, Zhukov A, GrossingerR, Gonzalez J. J Magn Magn Mater, 1999; 203: 292 [7] Kwon H S, Lee H, Kim K, Yu S C, Kim Y K. J AlloysCompd, 2001; 326: 309 [8] Xiao S Q, Liu Y H, Yan S S, Dai Y Y, Zhang L, Mei LM. Phys Rev, 2000; 61B: 5734 [9] Sommer R L, Chien C L. Appl Phys Lett, 1995; 67: 3346 [10] Huang G X, Xia Z H, Jin H J, Zhang Y Z. Met FundMater, 2001; 8: 27 (黄钢祥,夏朝晖,金惠娟,张延忠.金属功能材料,2001;8: 27)6 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|