Abstract Bulk Ti--Zr--Ni quasicrystals (QCs) were prepared by using conventional suction casting method. The characterization on their mechanical properties has been carried out by means of indentation and compression tests at room temperature. The strength indices of the icosahedral phase (I--phase)—based duplex phase alloy (α--Ti(Zr)+I phase) are 5.5 GPa in hardness and 1000 MPa in fracture strength, respectively. The Young's modulus is in the range of 23---36 GPa. The as--castTi60Zr25Ni15 QC--based composite alloy exhibits an elastic deformation capability of 4.2 % under a monaxial compression, which is about 4 times as large as that of Al—based QCs. The quasi--cleavage fracture morphologies indicate the bulk QC--based composite alloys to be brittle fracture.
|
|
Received: 20 January 2003
|
|
|
[1] Dubois J M. Mater Sci Eng, 2000; 294-296A: 4 [2] Nicula R, Jianu A, Ponkratz U, Burkel E. Phys Rev, 2000; 62B: 8844 [3] Ponkratz U, Nicula R, Jianu A, Burkel E. Ferroelectrics, 2001; 250:269 [4] Ponkratz U, Nicula R, Jianu A, Burkel E. J Phys, 2000;12:8071 [5] Foster K, Leisure R G, Shaklee J B, Kim J Y, Kelton K F. Phys Rev, 2000; 61B: 241 [6] Qiang J B, Wang Y M, Wang D H, Kramer M J, Dong C. J Non-Crystlline Solids, 2003; in Press [7] Qiang J B, Wang Y M, Wang D H, Kramer M J. Philos Mag Lett, 2003; 83:467 [8] Sigl L S, Mataga P A, Dalgleish B J, Meecking R M, Evans A G. Acta Metal Mater, 1988; 36:945 [9] Cahn J W, Shechtman D, Gratias D. J Mater Res, 1986; 1:13 [10] Bresson L. In: Hippert F, Gratias D eds., Lectures on Quasicrystals. Les Ulis: Les Editios de Physique, 1994: 549 [11] Koster U, Liebertz H, Liu W. Mater Sci Eng, 1994: 181-182A: 777 [12] Dong C. Quasicrystalline Materials. Beijing: National Defence Industry Press, 1998:159(董闯.准晶材料.北京:国防工业出版社,1998:159) [13] Zhang T, Inoue A. Mater Trans JIM, 1998; 39:1230 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|