Acta Metall Sin  2003, Vol. 39 Issue (6): 644-648     DOI:
Research Articles Current Issue | Archive | Adv Search |
Cite this article: 

. . Acta Metall Sin, 2003, 39(6): 644-648 .

Download:  PDF(217KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  15 August 2002     
ZTFLH:  TG171.44  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I6/644

[1] Li Y S, Niu Y, Wu W T. Corr Sci Prot Technol, 2000; 12: 224(李远士,牛焱,吴维(山文).腐蚀科学与防护技术,2000;12:224)
[2] Spiegel M. Mater Corr, 1999; 50: 373
[3] Kawahara Y. Corr Sci, 2002; 44: 223
[4] Jegede A, Vasantasree V, Hocking M G. J Mater Sci Lett, 1995; 14: 1089
[5] Jegede A, Vasantasree V, Hocking M G. J Mater Sci Lett, 1995; 14: 858
[6] Yao Z, Marek M. Mater Sci Eng A, 1995; 192-193: 994
[7] Li Y S, Wang F G, Niu Y, Wu W T. Rare Met Mater Eng, 2001; 30: 376(李远士,王富岗,牛焱,吴维(山文).稀有金属材料与工程,2001;30:376)
[8] Lee Y Y, McNallan M J. Metall Trans A, 1987; 18A(7) : 1099
[9] Shu Y H, Wang F H, Wu W T. Oxid Met, 1999; 52(5/6) : 463
[10] Sato Y, Young D J. Oxid Met, 2001; 55(3/4) : 243
[11] Jacobson N S. Oxid Met, 1986; 26: 157
[12] Spiegel M, Brabke H J. Mater Corr, 1995; 46: 121
[13] Hossain M K, Saunders S R J. Oxid Met, 1978; 12: 1
[14] Shinata Y, Hara M, Nakagawa T. JIM, 1991; 32: 969
[15] Ma H T, Wang L, Li Y S. J Mater Sci Technol, 2003; 19(5) , to be accepted
[16] Kanahara Y. Mater High Temp, 1997; 14: 261
[17] Kubaschewki O, Alcock C B. Metallugical Thermochemistry. 5th ed, Oxford, Pergamon Press, 1979: 377
[18] Sato Y, Hara M, Shinata Y. J Jpn Inst Met, 1996; 60: 192
[19] McNallan M J, Liang W W, Kim S H, Kang C T. In: Rapp R A ed, High Temperature Corrosion, NACE, Houston, Tex, USA, 1983: 316
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!