Please wait a minute...
Acta Metall Sin  2003, Vol. 39 Issue (2): 175-181     DOI:
Research Articles Current Issue | Archive | Adv Search |
Mechanical Properties of CO2 Corrosion Scale on N80 Well Tube Steel
CHEN Changfeng; LU Minxu; ZHAO Guoxian; BAI Zhenquan; YAN Milin; YANG Yanqing
School of Materials SCIENCE AND Engineering; University of Science and Technology; Beijing 100083
Cite this article: 

CHEN Changfeng; LU Minxu; ZHAO Guoxian; BAI Zhenquan; YAN Milin; YANG Yanqing. Mechanical Properties of CO2 Corrosion Scale on N80 Well Tube Steel. Acta Metall Sin, 2003, 39(2): 175-181 .

Download:  PDF(284KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  28 April 2002     
ZTFLH:  TG113.25  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2003/V39/I2/175

[1] Palacios C A, Shadley J R. Corrosion, 1991; 47: 122
[2] Dugstad A, Hemmer H, Seiersten M. Corrosion/2000, No.46, Houston, NACE, 2000
[3] Palacios C A, Shadley J R. Corrosion, 1993; 49: 686
[4] Seal S, Jepson W P, Gopal M. Corrosion/2000, No.46, Houston, NACE, 2000
[5] Ramachandran S, Campbell S, Ward M B. Corrosion/2000, No.25, Houston, NACE, 2000
[6] Gopal M, Rajappa S. Corrosion/1999, No.46, Houston, NACE, 1999
[7] Schmitt G A, Mueller M. Corrosion/1999, No.44, Houston, NACE, 1999:
[8] Schmitt G A, Mueller M. Corrosion/1999, No.88, Houston, NACE, 1999
[9] Stoney G G. Proc R Soc London, 1909; A82: 172
[10] Tian M P, Lin D Q. Science and Technology of Films. Beijing: China Machinery Press, 1991: 158(田民波,刘德令,编译,薄膜科学与技术.北京:机械工业出版社, 1991:1 58)
[11] Gou W X, Jin B S, Wei F. Mechanics of Materials. Xi'an: Northwestern Polytechnical University Press, 2000: 285(苟文选,金宝森,卫 丰,材料力学,西安:西北工业大学出版社,2000:285)
[12] Zhou Y, Lei T Q. Ceramic Material Science. Harbin: Harbin Institute of Technology Press, 1995: 369(周玉,雷廷权.陶瓷材料学.哈尔滨:哈尔滨工业大出版社,1995:369)
[13] Chen C F, Lu M X, Zhao G X, Yan M L, Bai Z Q, Yang Y Q. Acta Metall Sin, 2002; 38: 411(陈长风,路民旭,赵国仙,严密林,白真权,杨延清,金属学报,2002;38:411)
[14] Ueda M, Takabe H. Corrosion/2000, No.46, Houston,NACE, 2000
[15] Guo X Z, Gao K W, Qiao L J, Chu W Y. Acta Metall Sin,2000; 36: 753(郭献忠,高克玮,乔利杰,褚武扬.金属学报,2000;36:753)
[16] Liu G G, Cheng Q C. Shanghai Met, 2001; 23: 35(刘国光,程青蟾.上海金属, 2001;23:35)
[17] Chen C F, Zhao G X, Lu M X, Yang Y Q. Li H L. ./ Chin Sac Gorros Protect, 2002; 22: 143(陈长风,赵国仙,路民旭,杨延清,李鹤林.中国腐蚀与防护学报,2002;22:143)
[18] Jin Z Z, Bao Y W. Characterization of Mechanical Properties for Brittle Materials and Ceramics. Beijing: China Railway Press, 1996: 51(金子哲,包亦望,脆性材料力学性能评价与设计,北京:中国铁道出版社, 1996:51)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!